PURPOSE: The aim of the present study was to investigate the effects of surface treatments on the bond strengths between polymer-containing restorative materials and two dual-cure resin cements. MATERIALS AND METHODS: In the present study, rectangular samples prepared from Lava Ultimate (LU) and Vit...

Descripción completa

Detalles Bibliográficos
Autores principales: Turker, Nurullah, Buyukkaplan, Ulviye Şebnem, Başar, Ebru Kaya, Özarslan, Mehmet Mustafa
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Korean Academy of Prosthodontics 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7449818/
https://www.ncbi.nlm.nih.gov/pubmed/32879708
http://dx.doi.org/10.4047/jap.2020.12.4.189
Descripción
Sumario:PURPOSE: The aim of the present study was to investigate the effects of surface treatments on the bond strengths between polymer-containing restorative materials and two dual-cure resin cements. MATERIALS AND METHODS: In the present study, rectangular samples prepared from Lava Ultimate (LU) and Vita Enamic (VE) blocks were used. The specimen surfaces were treated using CoJet sandblasting, 50 µm Al(2)O(3) sandblasting, % 9 HF (hydrofluoric) acid, ER,Cr:YSGG laser treatment, and Z-Prime. Dual-cure resin cements (TheraCem and 3M RelyX U 200) were applied on each specimen's treated surface. A micro-tensile device was used to evaluate shear bond strength. Statistical analysis was performed using the SAS 9.4v3. RESULTS: While the bond strength using TheraCem with LU or VE was not statistically significant (P=.164), the bond strength using U200 with VE was statistically significant (P=.006). In the TheraCem applied VE groups, Z-Prime and HF acid were statistically different from CoJet, Laser, and Sandblast groups. In comparison of TheraCem used LU group, there was a statistically significant difference between HF acid and other surface treatments. CONCLUSION: The bonding performance between the restorative materials and cements were material type-dependent and surface treatment had a large effect on the bond strength. Within the limitations of the study, the use of both U200 and TheraCem may be suggested if Z-prime was applied to intaglio surfaces of VE. The cementation of LU using TheraCem is suitable after HF acid conditioning of the restoration surfaces.