Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study

This study evaluated the effect of incorporating silver nanoparticles (AgNPs) into conventional orthodontic adhesive on its antibacterial activity and the shear bond strength (SBS) to stainless steel orthodontic brackets. Thirty-four extracted premolars were randomly allocated into two groups (n = 1...

Descripción completa

Detalles Bibliográficos
Autores principales: Eslamian, Ladan, Borzabadi-Farahani, Ali, Karimi, Shahedeh, Saadat, Sepideh, Badiee, Mohammad Reza
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7466539/
https://www.ncbi.nlm.nih.gov/pubmed/32727028
http://dx.doi.org/10.3390/nano10081466
_version_ 1783577837001768960
author Eslamian, Ladan
Borzabadi-Farahani, Ali
Karimi, Shahedeh
Saadat, Sepideh
Badiee, Mohammad Reza
author_facet Eslamian, Ladan
Borzabadi-Farahani, Ali
Karimi, Shahedeh
Saadat, Sepideh
Badiee, Mohammad Reza
author_sort Eslamian, Ladan
collection PubMed
description This study evaluated the effect of incorporating silver nanoparticles (AgNPs) into conventional orthodontic adhesive on its antibacterial activity and the shear bond strength (SBS) to stainless steel orthodontic brackets. Thirty-four extracted premolars were randomly allocated into two groups (n = 17). Orthodontic adhesive (Transbond XT, 3M Unitek) was blended with AgNPs (50 nm, 0.3% w/w) to form a nano-adhesive. In order to bond stainless steel twin brackets (0.022-inch, American Orthodontics), Transbond XT (n = 17) and nano-adhesive (n = 17) were used in each group, respectively, after acid etching (37% phosphoric acid, 30 s) and rinsing with water (15 s). SBS and the adhesive remnant index (ARI) scores were recorded. Antibacterial activity against Streptococcus mutans in both groups after 24 h and 30 days was assessed (Disc agar diffusion test) and the inhibition zone diameter around each specimen was measured and recorded. Adding AgNPs significantly (p = 0.009) reduced the mean (SD) SBS in the nano-adhesive group [10.51(7.15) MPa] compared to Transbond XT [17.72(10.55) MPa]. The ARI scores on the Transbond XT and nano-adhesive showed no statistically significant difference (p = 0.322). Nano-adhesive with AgNPs showed significant antibacterial activity against Streptococcus mutans at 24 h and 30 days (p < 0.001). In both groups, no significant decline in the zones of inhibition was detected after 30 days (p = 0.907). The findings suggest that SBS decreased after incorporation of AgNPs [0.3% (w/w)], but was still above the recommended SBS of 5.9–7.8 MPa. The nano-adhesive showed significant antibacterial activity which did not change much after 30 days.
format Online
Article
Text
id pubmed-7466539
institution National Center for Biotechnology Information
language English
publishDate 2020
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-74665392020-09-14 Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study Eslamian, Ladan Borzabadi-Farahani, Ali Karimi, Shahedeh Saadat, Sepideh Badiee, Mohammad Reza Nanomaterials (Basel) Article This study evaluated the effect of incorporating silver nanoparticles (AgNPs) into conventional orthodontic adhesive on its antibacterial activity and the shear bond strength (SBS) to stainless steel orthodontic brackets. Thirty-four extracted premolars were randomly allocated into two groups (n = 17). Orthodontic adhesive (Transbond XT, 3M Unitek) was blended with AgNPs (50 nm, 0.3% w/w) to form a nano-adhesive. In order to bond stainless steel twin brackets (0.022-inch, American Orthodontics), Transbond XT (n = 17) and nano-adhesive (n = 17) were used in each group, respectively, after acid etching (37% phosphoric acid, 30 s) and rinsing with water (15 s). SBS and the adhesive remnant index (ARI) scores were recorded. Antibacterial activity against Streptococcus mutans in both groups after 24 h and 30 days was assessed (Disc agar diffusion test) and the inhibition zone diameter around each specimen was measured and recorded. Adding AgNPs significantly (p = 0.009) reduced the mean (SD) SBS in the nano-adhesive group [10.51(7.15) MPa] compared to Transbond XT [17.72(10.55) MPa]. The ARI scores on the Transbond XT and nano-adhesive showed no statistically significant difference (p = 0.322). Nano-adhesive with AgNPs showed significant antibacterial activity against Streptococcus mutans at 24 h and 30 days (p < 0.001). In both groups, no significant decline in the zones of inhibition was detected after 30 days (p = 0.907). The findings suggest that SBS decreased after incorporation of AgNPs [0.3% (w/w)], but was still above the recommended SBS of 5.9–7.8 MPa. The nano-adhesive showed significant antibacterial activity which did not change much after 30 days. MDPI 2020-07-27 /pmc/articles/PMC7466539/ /pubmed/32727028 http://dx.doi.org/10.3390/nano10081466 Text en © 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Eslamian, Ladan
Borzabadi-Farahani, Ali
Karimi, Shahedeh
Saadat, Sepideh
Badiee, Mohammad Reza
Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study
title Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study
title_full Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study
title_fullStr Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study
title_full_unstemmed Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study
title_short Evaluation of the Shear Bond Strength and Antibacterial Activity of Orthodontic Adhesive Containing Silver Nanoparticle, an In-Vitro Study
title_sort evaluation of the shear bond strength and antibacterial activity of orthodontic adhesive containing silver nanoparticle, an in-vitro study
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7466539/
https://www.ncbi.nlm.nih.gov/pubmed/32727028
http://dx.doi.org/10.3390/nano10081466
work_keys_str_mv AT eslamianladan evaluationoftheshearbondstrengthandantibacterialactivityoforthodonticadhesivecontainingsilvernanoparticleaninvitrostudy
AT borzabadifarahaniali evaluationoftheshearbondstrengthandantibacterialactivityoforthodonticadhesivecontainingsilvernanoparticleaninvitrostudy
AT karimishahedeh evaluationoftheshearbondstrengthandantibacterialactivityoforthodonticadhesivecontainingsilvernanoparticleaninvitrostudy
AT saadatsepideh evaluationoftheshearbondstrengthandantibacterialactivityoforthodonticadhesivecontainingsilvernanoparticleaninvitrostudy
AT badieemohammadreza evaluationoftheshearbondstrengthandantibacterialactivityoforthodonticadhesivecontainingsilvernanoparticleaninvitrostudy