The volatilization behaviour of typical fluorine-containing slag in steelmaking
It was taken as typical steelmaking fluorine-containing slag systems with the remelting electroslag, continuous casting mould flux and refining slag. The volatilization behaviour of each slag system was analysed by thermogravimetric (TG) and mass spectrometry (MS) detection. The results showed that...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7481700/ https://www.ncbi.nlm.nih.gov/pubmed/32968527 http://dx.doi.org/10.1098/rsos.200704 |
_version_ | 1783580660715225088 |
---|---|
author | Zhao, Zhongyu Zhao, Junxue Tan, Zexin Qu, Boqiao Cui, Yaru |
author_facet | Zhao, Zhongyu Zhao, Junxue Tan, Zexin Qu, Boqiao Cui, Yaru |
author_sort | Zhao, Zhongyu |
collection | PubMed |
description | It was taken as typical steelmaking fluorine-containing slag systems with the remelting electroslag, continuous casting mould flux and refining slag. The volatilization behaviour of each slag system was analysed by thermogravimetric (TG) and mass spectrometry (MS) detection. The results showed that the remelting electroslag volatilized significantly above 1300°C and the volatiles were mainly CaF(2), MgF(2) with a small amount of SiF(4) and AlF(3); the continuous casting mould flux volatilization was divided into two stages, in the first stage (500°C∼800°C), CaF(2) and Na(2)O reacted to form NaF, and in the second stage (greater than 1200°C), the CaF(2) evaporation was highlighted; for CaF(2)-CaO-based refining slag, the volatilization was the most significant at the eutectic point 84% CaF(2)–16% CaO, and the volatility can be reduced by adding 5% SiO(2). This research will be guiding significance for the composition and performance control of fluorine-containing slag and metallurgical environmental protection in the steelmaking process. |
format | Online Article Text |
id | pubmed-7481700 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2020 |
publisher | The Royal Society |
record_format | MEDLINE/PubMed |
spelling | pubmed-74817002020-09-22 The volatilization behaviour of typical fluorine-containing slag in steelmaking Zhao, Zhongyu Zhao, Junxue Tan, Zexin Qu, Boqiao Cui, Yaru R Soc Open Sci Chemistry It was taken as typical steelmaking fluorine-containing slag systems with the remelting electroslag, continuous casting mould flux and refining slag. The volatilization behaviour of each slag system was analysed by thermogravimetric (TG) and mass spectrometry (MS) detection. The results showed that the remelting electroslag volatilized significantly above 1300°C and the volatiles were mainly CaF(2), MgF(2) with a small amount of SiF(4) and AlF(3); the continuous casting mould flux volatilization was divided into two stages, in the first stage (500°C∼800°C), CaF(2) and Na(2)O reacted to form NaF, and in the second stage (greater than 1200°C), the CaF(2) evaporation was highlighted; for CaF(2)-CaO-based refining slag, the volatilization was the most significant at the eutectic point 84% CaF(2)–16% CaO, and the volatility can be reduced by adding 5% SiO(2). This research will be guiding significance for the composition and performance control of fluorine-containing slag and metallurgical environmental protection in the steelmaking process. The Royal Society 2020-08-26 /pmc/articles/PMC7481700/ /pubmed/32968527 http://dx.doi.org/10.1098/rsos.200704 Text en © 2020 The Authors. http://creativecommons.org/licenses/by/4.0/ http://creativecommons.org/licenses/by/4.0/http://creativecommons.org/licenses/by/4.0/Published by the Royal Society under the terms of the Creative Commons Attribution License http://creativecommons.org/licenses/by/4.0/, which permits unrestricted use, provided the original author and source are credited. |
spellingShingle | Chemistry Zhao, Zhongyu Zhao, Junxue Tan, Zexin Qu, Boqiao Cui, Yaru The volatilization behaviour of typical fluorine-containing slag in steelmaking |
title | The volatilization behaviour of typical fluorine-containing slag in steelmaking |
title_full | The volatilization behaviour of typical fluorine-containing slag in steelmaking |
title_fullStr | The volatilization behaviour of typical fluorine-containing slag in steelmaking |
title_full_unstemmed | The volatilization behaviour of typical fluorine-containing slag in steelmaking |
title_short | The volatilization behaviour of typical fluorine-containing slag in steelmaking |
title_sort | volatilization behaviour of typical fluorine-containing slag in steelmaking |
topic | Chemistry |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7481700/ https://www.ncbi.nlm.nih.gov/pubmed/32968527 http://dx.doi.org/10.1098/rsos.200704 |
work_keys_str_mv | AT zhaozhongyu thevolatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT zhaojunxue thevolatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT tanzexin thevolatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT quboqiao thevolatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT cuiyaru thevolatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT zhaozhongyu volatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT zhaojunxue volatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT tanzexin volatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT quboqiao volatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking AT cuiyaru volatilizationbehaviouroftypicalfluorinecontainingslaginsteelmaking |