Joining of Dissimilar Alloys Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.1Si Using Linear Friction Welding

Dissimilar joints between Ti-6Al-4V (Ti-64) and Ti-6Al-2Sn-4Zr-2Mo-0.1Si (Ti-6242) were manufactured using linear friction welding. The weld quality, in terms of the microstructure and mechanical properties, was investigated after stress relief annealing (SRA) at 750 °C for 2 h and compared with the...