Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC

The manufacturing of parts from nickel-based superalloy Alloy 247LC by laser powder bed fusion (L-PBF) is challenging, primarily owing to the alloy’s susceptibility to cracks. Apart from the cracks, voids created during the L-PBF process should also be minimized to produce dense parts. In this study...

Descripción completa

Detalles Bibliográficos
Autores principales: Adegoke, Olutayo, Andersson, Joel, Brodin, Håkan, Pederson, Robert
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7503919/
https://www.ncbi.nlm.nih.gov/pubmed/32859031
http://dx.doi.org/10.3390/ma13173770
_version_ 1783584503804985344
author Adegoke, Olutayo
Andersson, Joel
Brodin, Håkan
Pederson, Robert
author_facet Adegoke, Olutayo
Andersson, Joel
Brodin, Håkan
Pederson, Robert
author_sort Adegoke, Olutayo
collection PubMed
description The manufacturing of parts from nickel-based superalloy Alloy 247LC by laser powder bed fusion (L-PBF) is challenging, primarily owing to the alloy’s susceptibility to cracks. Apart from the cracks, voids created during the L-PBF process should also be minimized to produce dense parts. In this study, samples of Alloy 247LC were manufactured by L-PBF, several of which could be produced with voids and crack density close to zero. A statistical design of experiments was used to evaluate the influence of the process parameters, namely laser power, scanning speed, and hatch distance (inherent to the volumetric energy density) on void formation, crack density, and microhardness of the samples. The window of process parameters, in which minimum voids and/or cracks were present, was predicted. It was shown that the void content increased steeply at a volumetric energy density threshold below 81 [Formula: see text]. The crack density, on the other hand, increased steeply at a volumetric energy density threshold above 163 [Formula: see text]. The microhardness displayed a relatively low value in three samples which displayed the lowest volumetric energy density and highest void content. It was also observed that two samples, which displayed the highest volumetric energy density and crack density, demonstrated a relatively high microhardness; which could be a vital evidence in future investigations to determine the fundamental mechanism of cracking. The laser power was concluded to be the strongest and statistically most significant process parameter that influenced void formation and microhardness. The interaction of laser power and hatch distance was the strongest and most significant factor that influenced the crack density.
format Online
Article
Text
id pubmed-7503919
institution National Center for Biotechnology Information
language English
publishDate 2020
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-75039192020-09-27 Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC Adegoke, Olutayo Andersson, Joel Brodin, Håkan Pederson, Robert Materials (Basel) Article The manufacturing of parts from nickel-based superalloy Alloy 247LC by laser powder bed fusion (L-PBF) is challenging, primarily owing to the alloy’s susceptibility to cracks. Apart from the cracks, voids created during the L-PBF process should also be minimized to produce dense parts. In this study, samples of Alloy 247LC were manufactured by L-PBF, several of which could be produced with voids and crack density close to zero. A statistical design of experiments was used to evaluate the influence of the process parameters, namely laser power, scanning speed, and hatch distance (inherent to the volumetric energy density) on void formation, crack density, and microhardness of the samples. The window of process parameters, in which minimum voids and/or cracks were present, was predicted. It was shown that the void content increased steeply at a volumetric energy density threshold below 81 [Formula: see text]. The crack density, on the other hand, increased steeply at a volumetric energy density threshold above 163 [Formula: see text]. The microhardness displayed a relatively low value in three samples which displayed the lowest volumetric energy density and highest void content. It was also observed that two samples, which displayed the highest volumetric energy density and crack density, demonstrated a relatively high microhardness; which could be a vital evidence in future investigations to determine the fundamental mechanism of cracking. The laser power was concluded to be the strongest and statistically most significant process parameter that influenced void formation and microhardness. The interaction of laser power and hatch distance was the strongest and most significant factor that influenced the crack density. MDPI 2020-08-26 /pmc/articles/PMC7503919/ /pubmed/32859031 http://dx.doi.org/10.3390/ma13173770 Text en © 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Adegoke, Olutayo
Andersson, Joel
Brodin, Håkan
Pederson, Robert
Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC
title Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC
title_full Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC
title_fullStr Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC
title_full_unstemmed Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC
title_short Influence of Laser Powder Bed Fusion Process Parameters on Voids, Cracks, and Microhardness of Nickel-Based Superalloy Alloy 247LC
title_sort influence of laser powder bed fusion process parameters on voids, cracks, and microhardness of nickel-based superalloy alloy 247lc
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7503919/
https://www.ncbi.nlm.nih.gov/pubmed/32859031
http://dx.doi.org/10.3390/ma13173770
work_keys_str_mv AT adegokeolutayo influenceoflaserpowderbedfusionprocessparametersonvoidscracksandmicrohardnessofnickelbasedsuperalloyalloy247lc
AT anderssonjoel influenceoflaserpowderbedfusionprocessparametersonvoidscracksandmicrohardnessofnickelbasedsuperalloyalloy247lc
AT brodinhakan influenceoflaserpowderbedfusionprocessparametersonvoidscracksandmicrohardnessofnickelbasedsuperalloyalloy247lc
AT pedersonrobert influenceoflaserpowderbedfusionprocessparametersonvoidscracksandmicrohardnessofnickelbasedsuperalloyalloy247lc