In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture

The laser power bed fusion approach has been successfully employed to manufacture Mo(Si,Al)(2)-based composites through the selective laser melting of a MoSi(2)-30 wt.% AlSi10Mg mixture for high-temperature structural applications. Composites were manufactured by leveraging the in situ reaction of t...

Descripción completa

Detalles Bibliográficos
Autores principales: Minasyan, Tatevik, Aydinyan, Sofiya, Toyserkani, Ehsan, Hussainova, Irina
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7504486/
https://www.ncbi.nlm.nih.gov/pubmed/32842477
http://dx.doi.org/10.3390/ma13173720
_version_ 1783584635917172736
author Minasyan, Tatevik
Aydinyan, Sofiya
Toyserkani, Ehsan
Hussainova, Irina
author_facet Minasyan, Tatevik
Aydinyan, Sofiya
Toyserkani, Ehsan
Hussainova, Irina
author_sort Minasyan, Tatevik
collection PubMed
description The laser power bed fusion approach has been successfully employed to manufacture Mo(Si,Al)(2)-based composites through the selective laser melting of a MoSi(2)-30 wt.% AlSi10Mg mixture for high-temperature structural applications. Composites were manufactured by leveraging the in situ reaction of the components during printing at 150–300 W laser power, 500–1000 mm·s(−1) laser scanning speed, and 100–134 J·mm(−3) volumetric energy density. Microcomputed tomography scans indicated a negligible induced porosity throughout the specimens. The fully dense Mo(Si(1-x),Al(x))(2)-based composites, with hardness exceeding 545 HV1 and low roughness for both the top (horizontal) and side (vertical) surfaces, demonstrated that laser-based additive manufacturing can be exploited to create unique structures containing hexagonal Mo(Si(0.67)Al(0.33))(2).
format Online
Article
Text
id pubmed-7504486
institution National Center for Biotechnology Information
language English
publishDate 2020
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-75044862020-09-24 In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture Minasyan, Tatevik Aydinyan, Sofiya Toyserkani, Ehsan Hussainova, Irina Materials (Basel) Article The laser power bed fusion approach has been successfully employed to manufacture Mo(Si,Al)(2)-based composites through the selective laser melting of a MoSi(2)-30 wt.% AlSi10Mg mixture for high-temperature structural applications. Composites were manufactured by leveraging the in situ reaction of the components during printing at 150–300 W laser power, 500–1000 mm·s(−1) laser scanning speed, and 100–134 J·mm(−3) volumetric energy density. Microcomputed tomography scans indicated a negligible induced porosity throughout the specimens. The fully dense Mo(Si(1-x),Al(x))(2)-based composites, with hardness exceeding 545 HV1 and low roughness for both the top (horizontal) and side (vertical) surfaces, demonstrated that laser-based additive manufacturing can be exploited to create unique structures containing hexagonal Mo(Si(0.67)Al(0.33))(2). MDPI 2020-08-23 /pmc/articles/PMC7504486/ /pubmed/32842477 http://dx.doi.org/10.3390/ma13173720 Text en © 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Minasyan, Tatevik
Aydinyan, Sofiya
Toyserkani, Ehsan
Hussainova, Irina
In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture
title In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture
title_full In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture
title_fullStr In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture
title_full_unstemmed In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture
title_short In Situ Mo(Si,Al)(2)-Based Composite through Selective Laser Melting of a MoSi(2)-30 wt.% AlSi10Mg Mixture
title_sort in situ mo(si,al)(2)-based composite through selective laser melting of a mosi(2)-30 wt.% alsi10mg mixture
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7504486/
https://www.ncbi.nlm.nih.gov/pubmed/32842477
http://dx.doi.org/10.3390/ma13173720
work_keys_str_mv AT minasyantatevik insitumosial2basedcompositethroughselectivelasermeltingofamosi230wtalsi10mgmixture
AT aydinyansofiya insitumosial2basedcompositethroughselectivelasermeltingofamosi230wtalsi10mgmixture
AT toyserkaniehsan insitumosial2basedcompositethroughselectivelasermeltingofamosi230wtalsi10mgmixture
AT hussainovairina insitumosial2basedcompositethroughselectivelasermeltingofamosi230wtalsi10mgmixture