Microstructure Evolution and Mechanical Properties of FeCoCrNiCuTi(0.8) High-Entropy Alloy Prepared by Directional Solidification

A CoCrCuFeNiTi(0.8) high-entropy alloy was prepared using directional solidification techniques at different withdrawal rates (50 μm/s, 100 μm/s, 500 μm/s). The results showed that the microstructure was dendritic at all withdrawal rates. As the withdrawal rate increased, the dendrite orientation be...