Erroneous or Arrhenius: A Degradation Rate-Based Model for EPDM during Homogeneous Ageing
To improve the predictive capability of long-term stress relaxation of elastomers during thermo-oxidative ageing, a method to separate reversible and irreversible processes was adopted. The separation is performed through the analysis of compression set after tempering. On the basis of this separati...
Autores principales: | Zaghdoudi, Maha, Kömmling, Anja, Jaunich, Matthias, Wolff, Dietmar |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7569797/ https://www.ncbi.nlm.nih.gov/pubmed/32967281 http://dx.doi.org/10.3390/polym12092152 |
Ejemplares similares
-
Scission, Cross-Linking, and Physical Relaxation during Thermal Degradation of Elastomers
por: Zaghdoudi, Maha, et al.
Publicado: (2019) -
Analysis of O-Ring Seal Failure under Static Conditions and Determination of End-of-Lifetime Criterion
por: Kömmling, Anja, et al.
Publicado: (2019) -
Effect of the Strain Rate on Damage in Filled EPDM during Single and Cyclic Loadings
por: Candau, Nicolas, et al.
Publicado: (2020) -
Erroneous
Publicado: (1883) -
Synthesis and properties of EPDM-based oil-absorptive gels with different types of EPDM and styrene derivatives
por: Zhang, Minghua, et al.
Publicado: (2021)