Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths

Four-armed poly(ε-caprolactone)-block-poly(d-lactide) (4-C-D) copolymers with different poly(d-lactide) (PDLA) block lengths (M(n,PDLA)s) were synthesized by sequential ring-opening polymerization (ROP). The formation of stereocomplex (SC) crystallites in the 80/20 poly(l-lactide) (PLLA)/4-C-D blend...

Descripción completa

Detalles Bibliográficos
Autores principales: Dai, Suyang, Wang, Min, Zhuang, Zhuoxin, Ning, Zhenbo
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7599906/
https://www.ncbi.nlm.nih.gov/pubmed/32992889
http://dx.doi.org/10.3390/polym12102195
_version_ 1783602997165555712
author Dai, Suyang
Wang, Min
Zhuang, Zhuoxin
Ning, Zhenbo
author_facet Dai, Suyang
Wang, Min
Zhuang, Zhuoxin
Ning, Zhenbo
author_sort Dai, Suyang
collection PubMed
description Four-armed poly(ε-caprolactone)-block-poly(d-lactide) (4-C-D) copolymers with different poly(d-lactide) (PDLA) block lengths (M(n,PDLA)s) were synthesized by sequential ring-opening polymerization (ROP). The formation of stereocomplex (SC) crystallites in the 80/20 poly(l-lactide) (PLLA)/4-C-D blends were investigated with the change of M(n,PDLA) from 0.5 to 1.5 kg/mol. It was found that the crystallization and alkaline degradation of the blends were profoundly affected by the formed SC crystallites. The PLLA/4-C-D0.5 blend had the lowest crystallization rate of the three blends, and it was difficult to see spherulites in this blend by polarized optical microscopy (POM) observation after isothermal crystallization at 140 °C for 4 h. Meanwhile, when M(n,PDLA) was 1 kg/mol or 1.5 kg/mol, SC crystallites could be formed in the PLLA/4-C-D blend and acted as nucleators for the crystallization of PLLA homo-crystals. However, the overall crystallization rates of the two blends were still lower than that of the neat PLLA. In the PLLA/4-C-D1.5 blend, the Raman results showed that small isolated SC spherulites were trapped inside the big PLLA homo-spherulites during isothermal crystallization. The degradation rate of the PLLA/4-C-D blend decreased when M(n,PDLA) increased from 0.5 to 1.5 kg/mol, and the degradation morphologies had a close relationship with the crystallization state of the blends. This work revealed the gradual formation of SC crystallites with the increase in M(n,PDLA) in the PLLA/4-C-D blends and its significant effect on the crystallization and degradation behaviors of the blend films.
format Online
Article
Text
id pubmed-7599906
institution National Center for Biotechnology Information
language English
publishDate 2020
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-75999062020-11-01 Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths Dai, Suyang Wang, Min Zhuang, Zhuoxin Ning, Zhenbo Polymers (Basel) Article Four-armed poly(ε-caprolactone)-block-poly(d-lactide) (4-C-D) copolymers with different poly(d-lactide) (PDLA) block lengths (M(n,PDLA)s) were synthesized by sequential ring-opening polymerization (ROP). The formation of stereocomplex (SC) crystallites in the 80/20 poly(l-lactide) (PLLA)/4-C-D blends were investigated with the change of M(n,PDLA) from 0.5 to 1.5 kg/mol. It was found that the crystallization and alkaline degradation of the blends were profoundly affected by the formed SC crystallites. The PLLA/4-C-D0.5 blend had the lowest crystallization rate of the three blends, and it was difficult to see spherulites in this blend by polarized optical microscopy (POM) observation after isothermal crystallization at 140 °C for 4 h. Meanwhile, when M(n,PDLA) was 1 kg/mol or 1.5 kg/mol, SC crystallites could be formed in the PLLA/4-C-D blend and acted as nucleators for the crystallization of PLLA homo-crystals. However, the overall crystallization rates of the two blends were still lower than that of the neat PLLA. In the PLLA/4-C-D1.5 blend, the Raman results showed that small isolated SC spherulites were trapped inside the big PLLA homo-spherulites during isothermal crystallization. The degradation rate of the PLLA/4-C-D blend decreased when M(n,PDLA) increased from 0.5 to 1.5 kg/mol, and the degradation morphologies had a close relationship with the crystallization state of the blends. This work revealed the gradual formation of SC crystallites with the increase in M(n,PDLA) in the PLLA/4-C-D blends and its significant effect on the crystallization and degradation behaviors of the blend films. MDPI 2020-09-25 /pmc/articles/PMC7599906/ /pubmed/32992889 http://dx.doi.org/10.3390/polym12102195 Text en © 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Dai, Suyang
Wang, Min
Zhuang, Zhuoxin
Ning, Zhenbo
Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths
title Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths
title_full Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths
title_fullStr Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths
title_full_unstemmed Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths
title_short Crystallization and Alkaline Degradation Behaviors of Poly(l-Lactide)/4-Armed Poly(ε-Caprolactone)-Block-Poly(d-Lactide) Blends with Different Poly(d-Lactide) Block Lengths
title_sort crystallization and alkaline degradation behaviors of poly(l-lactide)/4-armed poly(ε-caprolactone)-block-poly(d-lactide) blends with different poly(d-lactide) block lengths
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7599906/
https://www.ncbi.nlm.nih.gov/pubmed/32992889
http://dx.doi.org/10.3390/polym12102195
work_keys_str_mv AT daisuyang crystallizationandalkalinedegradationbehaviorsofpolyllactide4armedpolyecaprolactoneblockpolydlactideblendswithdifferentpolydlactideblocklengths
AT wangmin crystallizationandalkalinedegradationbehaviorsofpolyllactide4armedpolyecaprolactoneblockpolydlactideblendswithdifferentpolydlactideblocklengths
AT zhuangzhuoxin crystallizationandalkalinedegradationbehaviorsofpolyllactide4armedpolyecaprolactoneblockpolydlactideblendswithdifferentpolydlactideblocklengths
AT ningzhenbo crystallizationandalkalinedegradationbehaviorsofpolyllactide4armedpolyecaprolactoneblockpolydlactideblendswithdifferentpolydlactideblocklengths