Comparative Evaluation of Carbon Reinforced Polyetherketone Acetabular Cup using Finite Element Analysis

BACKGROUND: Patients suffering from osteoarthritis undergo surgery to replace hip joints with hip prosthesis implants. Today most acetabular cups of hip prostheses are made of Ultra-High-Molecular-Weight-Polyethylene. However, these materials acting as acetabular cups of the implant have been recall...

Descripción completa

Detalles Bibliográficos
Autores principales: A., Abdal, R., Noorani, G., Cha
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Shiraz University of Medical Sciences 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7753250/
https://www.ncbi.nlm.nih.gov/pubmed/33364214
http://dx.doi.org/10.31661/jbpe.v0i0.2005-1123
Descripción
Sumario:BACKGROUND: Patients suffering from osteoarthritis undergo surgery to replace hip joints with hip prosthesis implants. Today most acetabular cups of hip prostheses are made of Ultra-High-Molecular-Weight-Polyethylene. However, these materials acting as acetabular cups of the implant have been recalled since patients have been feeling uncomfortable and abstained from physical activities. A newly introduced material, 30% Carbon Reinforced Polyetherketone, possess better isotropic mechanical properties and lower wear rates. OBJECTIVE: The research aims to compare the von-Mises stresses and deformation in static and dynamic loading of Ultra-High Molecular-Weight-Polyethylene to 30% Reinforced Carbon Fiber Polyetherketone using Finite Element Analysis. MATERIAL AND METHODS: An analytical study was performed to evaluate material selection and their contact performances of acetabular cups. Four pairs have been analyzed under loading conditions following ASTM F2996-13 and ISO 7206-4 standards. The acetabular cups options are made of 30% Carbon Reinforced Fiber Polyetherketone or Ultra-High-Molecular-Weight-Polyethylene. Besides, the femoral head and steam options are either Alumina Ceramic or Cobalt Chrome Molybdenum. RESULTS: The yield strength of Ultra-High-Molecular-Weight-Polyethylene is considerably small, resulting in the acetabular cup to fail when applied to high loading conditions. Carbon Reinforced Polyetherketone with Alumina Ceramic yielded 65% lower deformation at stumbling phase. CONCLUSION: Since the study focuses on linear isotropic material properties, Alumina Ceramic dominates a higher elastic modulus than Cobalt Chrome Molybdenum, nominating it the best fit combination for lower von-Mises stresses, acting on the Carbon Reinforced Polyetherketone acetabular cup.