Cargando…
Influence of High-Temperature Oxidation and Test Conditions on the Dynamic Mechanical Properties of 2.5D SiC(f)/SiC(m) Composites
The influence of microstructure evolution on the dynamic mechanical properties, including storage modulus and internal friction, of the 2.5D SiC(f)/SiC(m) composites after high-temperature treatment (800 °C and 1400 °C) in the air was investigated by three-point bending vibration test. The effects o...
Autores principales: | Yang, Chenxi, Wu, Jiejie, Ditta, Allah, Wu, Sujun, Zhao, Zihua |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7795653/ https://www.ncbi.nlm.nih.gov/pubmed/33396241 http://dx.doi.org/10.3390/ma14010145 |
Ejemplares similares
-
Comparative Study on Micro-Grinding Performance of 2.5D C(f)/SiCs, 2.5D SiC(f)/SiCs, and SiC Ceramics
por: Wen, Quan, et al.
Publicado: (2023) -
αSiC - βSiC - graphene composites
por: Razmjoo, Ali, et al.
Publicado: (2023) -
Microstructural Analysis of Novel Preceramic Paper-Derived SiC(f)/SiC Composites
por: Li, Ke, et al.
Publicado: (2021) -
Significant Improvement of Mechanical Properties of SiC-Nanowire-Reinforced SiC(f)/SiC Composites via Atomic Deposition of Ni Catalysts
por: Wu, Zongxu, et al.
Publicado: (2022) -
Interfacial properties of SiC(f)/SiC minicomposites with a scheelite coating
por: Ni, Na, et al.
Publicado: (2022)