Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy
The low plasticity of high strength Mg-Gd-Y alloy has become the main obstacle to its application in engineering. In this paper, the origin, propagation and fracture processes of cracks of a solution of treated Mg-13Gd-5Y-3Zn-0.3Zr alloy were observed and studied with scanning electron microscopy (S...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2020
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7795689/ https://www.ncbi.nlm.nih.gov/pubmed/33374133 http://dx.doi.org/10.3390/ma14010036 |
_version_ | 1783634504335753216 |
---|---|
author | Yang, Yaqin Mu, Chongli Han, Zhongjian Xu, Jian Li, Baocheng |
author_facet | Yang, Yaqin Mu, Chongli Han, Zhongjian Xu, Jian Li, Baocheng |
author_sort | Yang, Yaqin |
collection | PubMed |
description | The low plasticity of high strength Mg-Gd-Y alloy has become the main obstacle to its application in engineering. In this paper, the origin, propagation and fracture processes of cracks of a solution of treated Mg-13Gd-5Y-3Zn-0.3Zr alloy were observed and studied with scanning electron microscopy (SEM) in an in situ tensile test to provide theoretical references for the development of a new high-performance Mg-Gd-Y alloy. The results showed that there was still some bulk long period stacking order (LPSO) phase remaining in solid solution Mg-13Gd-5Y-3Zn-0.3Zr alloy. Most importantly, it was found that the locations of micro-cracks vary with the different solution treatment processes, mainly including the following three types. (1) At 480 × 10 h and 510 °C × 10 h, much bulk LPSO phase with higher elastic modulus remains in the alloy, which can lead to micro-cracks in the LPSO phase due to stress concentration. (2) At 510 °C × 13 h and 510 °C × 16 h, the phase structure of bulk LPSO changes, and the stress concentration easily appears at the LPSO/α-Mg interface, which leads to micro-cracks at the interface. (3) At 510 °C × 19 h and 510 °C × 22 h, the grain size increases, and the stress concentration is obvious at the grain boundary of coarse grains, which leads to the formation of micro-cracks. |
format | Online Article Text |
id | pubmed-7795689 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2020 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-77956892021-01-10 Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy Yang, Yaqin Mu, Chongli Han, Zhongjian Xu, Jian Li, Baocheng Materials (Basel) Article The low plasticity of high strength Mg-Gd-Y alloy has become the main obstacle to its application in engineering. In this paper, the origin, propagation and fracture processes of cracks of a solution of treated Mg-13Gd-5Y-3Zn-0.3Zr alloy were observed and studied with scanning electron microscopy (SEM) in an in situ tensile test to provide theoretical references for the development of a new high-performance Mg-Gd-Y alloy. The results showed that there was still some bulk long period stacking order (LPSO) phase remaining in solid solution Mg-13Gd-5Y-3Zn-0.3Zr alloy. Most importantly, it was found that the locations of micro-cracks vary with the different solution treatment processes, mainly including the following three types. (1) At 480 × 10 h and 510 °C × 10 h, much bulk LPSO phase with higher elastic modulus remains in the alloy, which can lead to micro-cracks in the LPSO phase due to stress concentration. (2) At 510 °C × 13 h and 510 °C × 16 h, the phase structure of bulk LPSO changes, and the stress concentration easily appears at the LPSO/α-Mg interface, which leads to micro-cracks at the interface. (3) At 510 °C × 19 h and 510 °C × 22 h, the grain size increases, and the stress concentration is obvious at the grain boundary of coarse grains, which leads to the formation of micro-cracks. MDPI 2020-12-24 /pmc/articles/PMC7795689/ /pubmed/33374133 http://dx.doi.org/10.3390/ma14010036 Text en © 2020 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Yang, Yaqin Mu, Chongli Han, Zhongjian Xu, Jian Li, Baocheng Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy |
title | Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy |
title_full | Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy |
title_fullStr | Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy |
title_full_unstemmed | Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy |
title_short | Analysis of the In Situ Crack Evolution Behavior in a Solid Solution Mg-13Gd-5Y-3Zn-0.3Zr Alloy |
title_sort | analysis of the in situ crack evolution behavior in a solid solution mg-13gd-5y-3zn-0.3zr alloy |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7795689/ https://www.ncbi.nlm.nih.gov/pubmed/33374133 http://dx.doi.org/10.3390/ma14010036 |
work_keys_str_mv | AT yangyaqin analysisoftheinsitucrackevolutionbehaviorinasolidsolutionmg13gd5y3zn03zralloy AT muchongli analysisoftheinsitucrackevolutionbehaviorinasolidsolutionmg13gd5y3zn03zralloy AT hanzhongjian analysisoftheinsitucrackevolutionbehaviorinasolidsolutionmg13gd5y3zn03zralloy AT xujian analysisoftheinsitucrackevolutionbehaviorinasolidsolutionmg13gd5y3zn03zralloy AT libaocheng analysisoftheinsitucrackevolutionbehaviorinasolidsolutionmg13gd5y3zn03zralloy |