Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones

The effect of a preliminary acid leaching for the recovery of gold by thiourea from printed circuit boards (PCBs) of spent mobile phones, was investigated. Preliminary leaching is aimed to recover copper in the leachate that would compete with gold in the successive leaching of the residue with thio...

Descripción completa

Detalles Bibliográficos
Autores principales: Ippolito, Nicolò Maria, Medici, Franco, Pietrelli, Loris, Piga, Luigi
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7828416/
https://www.ncbi.nlm.nih.gov/pubmed/33450981
http://dx.doi.org/10.3390/ma14020362
_version_ 1783641007446818816
author Ippolito, Nicolò Maria
Medici, Franco
Pietrelli, Loris
Piga, Luigi
author_facet Ippolito, Nicolò Maria
Medici, Franco
Pietrelli, Loris
Piga, Luigi
author_sort Ippolito, Nicolò Maria
collection PubMed
description The effect of a preliminary acid leaching for the recovery of gold by thiourea from printed circuit boards (PCBs) of spent mobile phones, was investigated. Preliminary leaching is aimed to recover copper in the leachate that would compete with gold in the successive leaching of the residue with thiourea, thus preventing the formation of the gold-thiourea complex. Two hydrometallurgical routes were tested for the recovery of copper first, and gold after. The first one was based on a two-step leaching that utilizes sulfuric acid and hydrogen peroxide in the preliminary leaching and then thiourea for the recovery of gold in the successive leaching: A copper and gold recovery of 81% and 79% were obtained, respectively. In the second route, nitric acid was used: 100% of copper was recovered in the leachate and 85% of gold in the thiourea successive leaching. The main operative parameters, namely thiourea and ferric sulphate concentrations, leach time, liquid-solid ratio, and temperature were studied according to a factorial plan strategy. A flowsheet of the processes was proposed, and a mass balance of both routes was obtained. Finally, qualitative considerations on the technical and economic feasibility of the different routes were made.
format Online
Article
Text
id pubmed-7828416
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-78284162021-01-25 Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones Ippolito, Nicolò Maria Medici, Franco Pietrelli, Loris Piga, Luigi Materials (Basel) Article The effect of a preliminary acid leaching for the recovery of gold by thiourea from printed circuit boards (PCBs) of spent mobile phones, was investigated. Preliminary leaching is aimed to recover copper in the leachate that would compete with gold in the successive leaching of the residue with thiourea, thus preventing the formation of the gold-thiourea complex. Two hydrometallurgical routes were tested for the recovery of copper first, and gold after. The first one was based on a two-step leaching that utilizes sulfuric acid and hydrogen peroxide in the preliminary leaching and then thiourea for the recovery of gold in the successive leaching: A copper and gold recovery of 81% and 79% were obtained, respectively. In the second route, nitric acid was used: 100% of copper was recovered in the leachate and 85% of gold in the thiourea successive leaching. The main operative parameters, namely thiourea and ferric sulphate concentrations, leach time, liquid-solid ratio, and temperature were studied according to a factorial plan strategy. A flowsheet of the processes was proposed, and a mass balance of both routes was obtained. Finally, qualitative considerations on the technical and economic feasibility of the different routes were made. MDPI 2021-01-13 /pmc/articles/PMC7828416/ /pubmed/33450981 http://dx.doi.org/10.3390/ma14020362 Text en © 2021 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Ippolito, Nicolò Maria
Medici, Franco
Pietrelli, Loris
Piga, Luigi
Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones
title Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones
title_full Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones
title_fullStr Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones
title_full_unstemmed Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones
title_short Effect of Acid Leaching Pre-Treatment on Gold Extraction from Printed Circuit Boards of Spent Mobile Phones
title_sort effect of acid leaching pre-treatment on gold extraction from printed circuit boards of spent mobile phones
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7828416/
https://www.ncbi.nlm.nih.gov/pubmed/33450981
http://dx.doi.org/10.3390/ma14020362
work_keys_str_mv AT ippolitonicolomaria effectofacidleachingpretreatmentongoldextractionfromprintedcircuitboardsofspentmobilephones
AT medicifranco effectofacidleachingpretreatmentongoldextractionfromprintedcircuitboardsofspentmobilephones
AT pietrelliloris effectofacidleachingpretreatmentongoldextractionfromprintedcircuitboardsofspentmobilephones
AT pigaluigi effectofacidleachingpretreatmentongoldextractionfromprintedcircuitboardsofspentmobilephones