Dissolution Kinetics of International Simple Glass and Formation of Secondary Phases at Very High Surface Area to Solution Ratio in Young Cement Water
Static dissolution experiments were carried out with the reference International Simple Glass under hyperalkaline pH at 70 °C and very high SA/V ratio. Three aspects of glass dissolution behavior were investigated, (1) the rate drop regime and the residual rate (stage II), (2) the formation of secon...
Autores principales: | Ferrand, Karine, Klinkenberg, Martina, Caes, Sébastien, Poonoosamy, Jenna, Van Renterghem, Wouter, Barthel, Juri, Lemmens, Karel, Bosbach, Dirk, Brandt, Felix |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC7961375/ https://www.ncbi.nlm.nih.gov/pubmed/33800843 http://dx.doi.org/10.3390/ma14051254 |
Ejemplares similares
-
Structure and dissolution of silicophosphate glass
por: Takada, Kazuya, et al.
Publicado: (2022) -
A lab-on-a-chip approach integrating in-situ characterization and reactive transport modelling diagnostics to unravel (Ba,Sr)SO(4) oscillatory zoning
por: Poonoosamy, Jenna, et al.
Publicado: (2021) -
Microfluidic investigation of pore-size dependency of barite nucleation
por: Poonoosamy, Jenna, et al.
Publicado: (2023) -
Kinetics of ion release from a conventional glass-ionomer cement
por: Nicholson, John W., et al.
Publicado: (2021) -
Early-Stage Dissolution Kinetics of Silicate-Based Bioactive Glass under Dynamic Conditions: Critical Evaluation
por: Galusková, Dagmar, et al.
Publicado: (2021)