A Simple Method for a Protective Coating on Stainless Steel against Molten Aluminum Alloy Comprising Polymer-Derived Ceramics, Oxides and Refractory Ceramics

A new coating based on polymer-derived ceramics (PDC), oxides and refractory ceramic with a thickness of around 50 µm has been developed to improve the resistance corrosion of stainless steel substrate against molten aluminum alloy in a thermal energy storage (TES) system designed to run at high tem...

Descripción completa

Detalles Bibliográficos
Autores principales: Quenard, Sébastien, Roumanie, Marilyne
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8003667/
https://www.ncbi.nlm.nih.gov/pubmed/33808939
http://dx.doi.org/10.3390/ma14061519
Descripción
Sumario:A new coating based on polymer-derived ceramics (PDC), oxides and refractory ceramic with a thickness of around 50 µm has been developed to improve the resistance corrosion of stainless steel substrate against molten aluminum alloy in a thermal energy storage (TES) system designed to run at high temperature (up to 600 °C). These coatings implemented by straightforward methods, like tape casting or paintbrush, were coated on planar and cylindrical stainless-steel substrates, pyrolyzed at 700 °C before being plunged for 600 and 1200 h in molten AlSi(12) at 700 °C. The stainless-steel substrate appears healthy without intermetallic compounds, characteristic of molten aluminum alloy corrosion. The protective coating against AlSi(12) corrosion shows excellent performance and appears interesting for TES applications.