Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate

With a telluride-type gold ore flotation concentrate as the research object, the Na(2)S + NaOH collaborative leaching process was applied to selectively separate tellurium before the cyanide leaching of gold and silver. The effects of process parameters including the type of leaching agent, the amou...

Descripción completa

Detalles Bibliográficos
Autores principales: Yang, Wei, Lan, Xuechen, Wang, Qian, Dong, Ping, Wang, Gang
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Frontiers Media S.A. 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8027068/
https://www.ncbi.nlm.nih.gov/pubmed/33842428
http://dx.doi.org/10.3389/fchem.2021.593888
_version_ 1783675748306911232
author Yang, Wei
Lan, Xuechen
Wang, Qian
Dong, Ping
Wang, Gang
author_facet Yang, Wei
Lan, Xuechen
Wang, Qian
Dong, Ping
Wang, Gang
author_sort Yang, Wei
collection PubMed
description With a telluride-type gold ore flotation concentrate as the research object, the Na(2)S + NaOH collaborative leaching process was applied to selectively separate tellurium before the cyanide leaching of gold and silver. The effects of process parameters including the type of leaching agent, the amount of leaching agent, liquid-solid ratio, leaching temperature, and leaching time on the leaching rate of tellurium were investigated. The results showed that the tellurium leaching rate could reach 78.14% under the optimum conditions of −0.038 mm (95%) grinding fineness, 80 g/L Na(2)S concentration, 30 g/L NaOH concentration, 4:1 liquid-solid ratio, 80°C leaching temperature and 3 h′s leaching time. The kinetic analysis showed that the leaching process of tellurium from telluride-type gold concentrate was a mixed type of chemical reaction control and diffusion control. The grain parameter in the leaching process was 0.26263 and the apparent activation energy E = 17.12 kJ/mol. Tellurium could be pre-leached from the telluride-type gold flotation concentrate through the Na(2)S + NaOH alkaline leaching process to achieve the effective separation of tellurium from noble metals, which, when eliminating the adverse effects of telluride on the leaching of gold and silver, provides new ideas for the extraction of rare element tellurium.
format Online
Article
Text
id pubmed-8027068
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher Frontiers Media S.A.
record_format MEDLINE/PubMed
spelling pubmed-80270682021-04-09 Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate Yang, Wei Lan, Xuechen Wang, Qian Dong, Ping Wang, Gang Front Chem Chemistry With a telluride-type gold ore flotation concentrate as the research object, the Na(2)S + NaOH collaborative leaching process was applied to selectively separate tellurium before the cyanide leaching of gold and silver. The effects of process parameters including the type of leaching agent, the amount of leaching agent, liquid-solid ratio, leaching temperature, and leaching time on the leaching rate of tellurium were investigated. The results showed that the tellurium leaching rate could reach 78.14% under the optimum conditions of −0.038 mm (95%) grinding fineness, 80 g/L Na(2)S concentration, 30 g/L NaOH concentration, 4:1 liquid-solid ratio, 80°C leaching temperature and 3 h′s leaching time. The kinetic analysis showed that the leaching process of tellurium from telluride-type gold concentrate was a mixed type of chemical reaction control and diffusion control. The grain parameter in the leaching process was 0.26263 and the apparent activation energy E = 17.12 kJ/mol. Tellurium could be pre-leached from the telluride-type gold flotation concentrate through the Na(2)S + NaOH alkaline leaching process to achieve the effective separation of tellurium from noble metals, which, when eliminating the adverse effects of telluride on the leaching of gold and silver, provides new ideas for the extraction of rare element tellurium. Frontiers Media S.A. 2021-03-25 /pmc/articles/PMC8027068/ /pubmed/33842428 http://dx.doi.org/10.3389/fchem.2021.593888 Text en Copyright © 2021 Yang, Lan, Wang, Dong and Wang. https://creativecommons.org/licenses/by/4.0/This is an open-access article distributed under the terms of the Creative Commons Attribution License (CC BY). The use, distribution or reproduction in other forums is permitted, provided the original author(s) and the copyright owner(s) are credited and that the original publication in this journal is cited, in accordance with accepted academic practice. No use, distribution or reproduction is permitted which does not comply with these terms.
spellingShingle Chemistry
Yang, Wei
Lan, Xuechen
Wang, Qian
Dong, Ping
Wang, Gang
Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate
title Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate
title_full Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate
title_fullStr Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate
title_full_unstemmed Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate
title_short Selective Pre-leaching of Tellurium From Telluride-Type Gold Concentrate
title_sort selective pre-leaching of tellurium from telluride-type gold concentrate
topic Chemistry
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8027068/
https://www.ncbi.nlm.nih.gov/pubmed/33842428
http://dx.doi.org/10.3389/fchem.2021.593888
work_keys_str_mv AT yangwei selectivepreleachingoftelluriumfromtelluridetypegoldconcentrate
AT lanxuechen selectivepreleachingoftelluriumfromtelluridetypegoldconcentrate
AT wangqian selectivepreleachingoftelluriumfromtelluridetypegoldconcentrate
AT dongping selectivepreleachingoftelluriumfromtelluridetypegoldconcentrate
AT wanggang selectivepreleachingoftelluriumfromtelluridetypegoldconcentrate