Permanent Deformation and Stiffness Degradation of Open Hole Glass/PA6 UD Thermoplastic Composite in Tension and Compression

UD glass/PA6 coupons with an open hole are subjected to tensile and compressive loading. Three layups: [0/90](5s), [+45/−45](5s) and [+45/0/−45/90](3s) with a shape based on ASTM D5766 were tested. Both monotonic loading as well as loading–unloading–reloading tests were executed. The strain field on...