Cargando…

Flexural Strength and Hardness of Filler-Reinforced PMMA Targeted for Denture Base Application

The aim of this work was to evaluate the flexural strength and surface hardness of heat-cured Polymethyl methacrylate (PMMA) modified by the addition of ZrO(2) nanoparticles, TiO(2) nanoparticles, and E-glass fibre at different wt.% concentrations. Specimens were fabricated and separated into four g...

Descripción completa

Detalles Bibliográficos
Autores principales: Alhotan, Abdulaziz, Yates, Julian, Zidan, Saleh, Haider, Julfikar, Silikas, Nikolaos
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8159135/
https://www.ncbi.nlm.nih.gov/pubmed/34069482
http://dx.doi.org/10.3390/ma14102659
Descripción
Sumario:The aim of this work was to evaluate the flexural strength and surface hardness of heat-cured Polymethyl methacrylate (PMMA) modified by the addition of ZrO(2) nanoparticles, TiO(2) nanoparticles, and E-glass fibre at different wt.% concentrations. Specimens were fabricated and separated into four groups (n = 10) to measure both flexural strength and surface hardness. Group C was the control group. The specimens in the remaining three groups differed according to the ratio of filler to weight of PMMA resin (1.5%, 3%, 5%, and 7%). A three-point bending test was performed to determine the flexural strength, while the surface hardness was measured using the Vickers hardness. Scanning Electron Microscope (SEM) was employed to observe the fractured surface of the specimens. The flexural strength was significantly improved in the groups filled with 3 wt.% ZrO(2) and 5 and 7 wt.% E-glass fibre in comparison to Group C. All the groups displayed a significantly higher surface hardness than Group C, with the exception of the 1.5% TiO(2) and 1.5% ZrO(2) groups. The optimal filler concentrations to enhance the flexural strength of PMMA resin were between 3–5% ZrO(2), 1.5% TiO(2), and 3–7% E-glass fibre. Furthermore, for all composites, a filler concentration of 3 wt.% and above would significantly improve hardness.