Cargando…

Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte

Potassium–selenium (K–Se) batteries offer fairly high theoretical voltage (∼1.88 V) and energy density (∼1275 W h kg(Se)(−1)). However, in practice, their operation voltage is so far limited to ∼1.4 V, resulting in insufficient energy utilization and mechanistic understanding. Here, it is demonstrat...

Descripción completa

Detalles Bibliográficos
Autores principales: Liu, Qin, Deng, Wenzhuo, Pan, Yilong, Sun, Chuan-Fu
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Royal Society of Chemistry 2020
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8159323/
https://www.ncbi.nlm.nih.gov/pubmed/34094097
http://dx.doi.org/10.1039/d0sc01474e
_version_ 1783700059702951936
author Liu, Qin
Deng, Wenzhuo
Pan, Yilong
Sun, Chuan-Fu
author_facet Liu, Qin
Deng, Wenzhuo
Pan, Yilong
Sun, Chuan-Fu
author_sort Liu, Qin
collection PubMed
description Potassium–selenium (K–Se) batteries offer fairly high theoretical voltage (∼1.88 V) and energy density (∼1275 W h kg(Se)(−1)). However, in practice, their operation voltage is so far limited to ∼1.4 V, resulting in insufficient energy utilization and mechanistic understanding. Here, it is demonstrated for the first time that K–Se batteries operating in concentrated ether-based electrolytes follow distinctive reaction pathways involving reversible stepwise conversion reactions from Se to K(2)Se(x) (x = 5, 3, 2, 1). The presence of redox intermediates K(2)Se(5) at ∼2.3 V and K(2)Se(3) at ∼2.1 V, in contrast with previous reports, enables record-high average discharge plateau voltage (1.85 V) and energy density (998 W h kg(Se)(−1) or 502 W h kg(K2Se)(−1)), both approaching the theoretical limits and surpassing those of previously reported Na/K/Al–Se batteries. Moreover, experimental analysis and first-principles calculations reveal that the effective suppression of detrimental polyselenide dissolution/shuttling in concentrated electrolytes, together with high electron conductibility of Se/K(2)Se(x), enables fast reaction kinetics, efficient utilization of Se, and long-term cyclability of up to 350 cycles, which are impracticable in either K–S counterparts or K–Se batteries with low/moderate-concentration electrolytes. This work may pave the way for mechanistic understanding and full energy utilization of K–Se battery chemistry.
format Online
Article
Text
id pubmed-8159323
institution National Center for Biotechnology Information
language English
publishDate 2020
publisher The Royal Society of Chemistry
record_format MEDLINE/PubMed
spelling pubmed-81593232021-06-04 Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte Liu, Qin Deng, Wenzhuo Pan, Yilong Sun, Chuan-Fu Chem Sci Chemistry Potassium–selenium (K–Se) batteries offer fairly high theoretical voltage (∼1.88 V) and energy density (∼1275 W h kg(Se)(−1)). However, in practice, their operation voltage is so far limited to ∼1.4 V, resulting in insufficient energy utilization and mechanistic understanding. Here, it is demonstrated for the first time that K–Se batteries operating in concentrated ether-based electrolytes follow distinctive reaction pathways involving reversible stepwise conversion reactions from Se to K(2)Se(x) (x = 5, 3, 2, 1). The presence of redox intermediates K(2)Se(5) at ∼2.3 V and K(2)Se(3) at ∼2.1 V, in contrast with previous reports, enables record-high average discharge plateau voltage (1.85 V) and energy density (998 W h kg(Se)(−1) or 502 W h kg(K2Se)(−1)), both approaching the theoretical limits and surpassing those of previously reported Na/K/Al–Se batteries. Moreover, experimental analysis and first-principles calculations reveal that the effective suppression of detrimental polyselenide dissolution/shuttling in concentrated electrolytes, together with high electron conductibility of Se/K(2)Se(x), enables fast reaction kinetics, efficient utilization of Se, and long-term cyclability of up to 350 cycles, which are impracticable in either K–S counterparts or K–Se batteries with low/moderate-concentration electrolytes. This work may pave the way for mechanistic understanding and full energy utilization of K–Se battery chemistry. The Royal Society of Chemistry 2020-05-25 /pmc/articles/PMC8159323/ /pubmed/34094097 http://dx.doi.org/10.1039/d0sc01474e Text en This journal is © The Royal Society of Chemistry https://creativecommons.org/licenses/by-nc/3.0/
spellingShingle Chemistry
Liu, Qin
Deng, Wenzhuo
Pan, Yilong
Sun, Chuan-Fu
Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte
title Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte
title_full Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte
title_fullStr Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte
title_full_unstemmed Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte
title_short Approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte
title_sort approaching the voltage and energy density limits of potassium–selenium battery chemistry in a concentrated ether-based electrolyte
topic Chemistry
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8159323/
https://www.ncbi.nlm.nih.gov/pubmed/34094097
http://dx.doi.org/10.1039/d0sc01474e
work_keys_str_mv AT liuqin approachingthevoltageandenergydensitylimitsofpotassiumseleniumbatterychemistryinaconcentratedetherbasedelectrolyte
AT dengwenzhuo approachingthevoltageandenergydensitylimitsofpotassiumseleniumbatterychemistryinaconcentratedetherbasedelectrolyte
AT panyilong approachingthevoltageandenergydensitylimitsofpotassiumseleniumbatterychemistryinaconcentratedetherbasedelectrolyte
AT sunchuanfu approachingthevoltageandenergydensitylimitsofpotassiumseleniumbatterychemistryinaconcentratedetherbasedelectrolyte