Cargando…

An In vitro Evaluation to Compare the Surface Roughness of Glazed, Reglazed and Chair Side Polished Surfaces of Dental Porcelain

AIM: The aim of this study was to evaluate the effect of glazing, reglazing, and chairside polishing on the surface roughness of dental porcelain. MATERIALS AND METHODS: A total of 50 discs of feldspathic porcelain were fabricated using a metal mold of dimension 10 mm × 2 mm. Based on the surface tr...

Descripción completa

Detalles Bibliográficos
Autores principales: Rani, Varsha, Mittal, Sanjeev, Sukhija, Urvashi
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Wolters Kluwer - Medknow 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8237812/
https://www.ncbi.nlm.nih.gov/pubmed/34220157
http://dx.doi.org/10.4103/ccd.ccd_86_20
Descripción
Sumario:AIM: The aim of this study was to evaluate the effect of glazing, reglazing, and chairside polishing on the surface roughness of dental porcelain. MATERIALS AND METHODS: A total of 50 discs of feldspathic porcelain were fabricated using a metal mold of dimension 10 mm × 2 mm. Based on the surface treatment, the samples were divided into five groups. Group A – Glazed (control), Group B – Abraded and reglazed, Group C – Abraded and polished with porcelain adjustment kit (Shofu Dental Corp. PN 0301 Classic Plastic HP Kit, Shofu Inc., Kyoto, Japan), Group D – Abraded and polished with diamond polishing paste (Shofu Dental Corp. PN 0558 DirectDia, Shofu Inc., Kyoto, Japan), Group E-Abraded and polished with the combination of porcelain adjustment kit followed by diamond polishing paste. The surface roughness (Ra) values (μm) were evaluated by a profilometer (Mitutoyo Surftest SJ-310, Tokyo, Japan). The data obtained were statistically analyzed using one-way ANOVA and post hoc Tukey's test. RESULTS: The mean surface roughness (Ra) of Groups A, B, C, D, and E was 0.567 ± 0.078 μm, 0.433 ± 0.059 μm, 0.882 ± 0.126 μm, 2.361 ± 0.195 μm, and 0.438 ± 0.043 μm, respectively. The samples of Group D (Polished with polishing paste alone) had the highest surface roughness (Ra value). Whereas the samples of Group B and E had similar surface roughness (Ra) value. Differences between Groups A, B, and E were statistically insignificant (P > 0.05). CONCLUSION: After adjustment of ceramic restorations in dental clinics, diamond polishing paste, when used after porcelain adjustment kit, could provide the marked finish equal to glazed or reglazed surface.