Impact of Prolonged Exposure of Eleven Years to Hot Seawater on the Degradation of a Thermoset Composite
This paper presents a long-term experimental investigation of E-glass/epoxy composites’ durability exposed to seawater at different temperatures. The thermoset composite samples were exposed to 23 °C, 45 °C and 65 °C seawater for a prolonged exposure time of 11 years. The mechanical performance as a...
Autores principales: | Idrisi, Amir Hussain, Mourad, Abdel-Hamid I., Sherif, Muhammad M. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8271879/ https://www.ncbi.nlm.nih.gov/pubmed/34208792 http://dx.doi.org/10.3390/polym13132154 |
Ejemplares similares
-
Investigation on the Durability of E-Glass/Epoxy Composite Exposed to Seawater at Elevated Temperature
por: Idrisi, Amir Hussain, et al.
Publicado: (2021) -
Utilization of Mechanically Recycled Carbon Fibers in Vinyl Ester Composites
por: AlHarmoodi, Khaled, et al.
Publicado: (2023) -
Prolonged Thermal Relaxation of the Thermosetting Polymers
por: Korolev, Alexander, et al.
Publicado: (2021) -
Seawater Absorption and Adhesion Properties of Hydrophobic and Superhydrophobic Thermoset Epoxy Nanocomposite Coatings
por: Atta, Ayman M., et al.
Publicado: (2021) -
Recycling of Thermoset Materials and Thermoset-Based Composites: Challenge and Opportunity
por: Morici, Elisabetta, et al.
Publicado: (2022)