Cargando…

Effect of a Powder Mould in the Post-Process Thermal Treatment of ABS Parts Manufactured with FDM Technology

The post-process thermal treatment of thermoplastics improves their mechanical properties, but causes deformations in parts, making them unusable. This work proposes a powder mould to prevent dimensional part deformation and studies the influence of line building direction in part deformations in a...

Descripción completa

Detalles Bibliográficos
Autores principales: Lluch-Cerezo, Joaquín, Benavente, Rut, Meseguer, María Desamparados, García-Manrique, Juan Antonio
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8347518/
https://www.ncbi.nlm.nih.gov/pubmed/34372026
http://dx.doi.org/10.3390/polym13152422
Descripción
Sumario:The post-process thermal treatment of thermoplastics improves their mechanical properties, but causes deformations in parts, making them unusable. This work proposes a powder mould to prevent dimensional part deformation and studies the influence of line building direction in part deformations in a post-process thermal treatment of 3D printed polymers. Two sets of ABS (acrylonitrile butadiene styrene) test samples manufactured by fused deposition modelling (FDM) in six different raster directions have been treated and evaluated. One set has been packed with a ceramic powder mould during thermal treatment to evaluate deformations and mould effectiveness. Thermogravimetric tests have been carried out on ABS samples, concluding that the thermal treatment of the samples does not cause degradations in the polymeric material. An analysis of variance (ANOVA) was performed to study internal building geometry and mould influence on part deformation after the thermal treatment. It can be concluded that powder mould considerably reduces dimensional deformations during the thermal treatment process, with length being the most affected dimension for deformation. Attending to the length, mould effectiveness is greater than 80% in comparison to non-usage of moulding, reaching 90% when the building lines are in the same direction as the main part.