The Influence of Different Surface Cleansing Agents on Shear Bond Strength of Contaminated Lithium Disilicate Ceramic: An In Vitro Study

MATERIALS AND METHODS: Seventy LDS specimens were randomly divided into seven groups. The first group was noncontaminated surface (PC). The six other groups were contaminated with the saliva and silicone disclosing medium and treated with no surface cleansing agent (NC); phosphoric acid (PO); Ivocle...

Descripción completa

Detalles Bibliográficos
Autores principales: Charasseangpaisarn, Taksid, Krassanairawiwong, Pattarawadee, Sangkanchanavanich, Chanidapa, Kurjirattikan, Atima, Kunyawatyuwapong, Kanyarak, Tantivasin, Natlada
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Hindawi 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8373498/
https://www.ncbi.nlm.nih.gov/pubmed/34422055
http://dx.doi.org/10.1155/2021/7112400
Descripción
Sumario:MATERIALS AND METHODS: Seventy LDS specimens were randomly divided into seven groups. The first group was noncontaminated surface (PC). The six other groups were contaminated with the saliva and silicone disclosing medium and treated with no surface cleansing agent (NC); phosphoric acid (PO); Ivoclean (IV); sodium hydroxide solution (NA); Restorative Cleansing Agent (RC); and hydrofluoric acid (HF). Then, LDS specimens were cementated with Panavia V5 to resin composite rod. Each specimen was subjected to an SBS test. The modes of failure was inspected under light microscope. The surface element of each group was examined by SEM-EDS. RESULTS: The results were analyzed with one-way ANOVA and Tamhane's T2. The mean SBS value of NC was significantly lower than others (p < 0.05), and HF was significantly higher than others (p < 0.05). However, PC, PO, IV, NA, and RC were not significantly different from each other (p > 0.05). The mode of failure was mostly adhesive failure in every group. The surface showed similar amount of elements in every group. CONCLUSIONS: The SBS of LDS was reduced by saliva and silicone disclosing medium contamination which can be restored using acid- and alkaline-based surface cleansing agents before the cementation procedure.