Poplar-based thermochromic composites that change colour at 38 °C to 46 °C
The red thermochromic dye (R-TD) is the tetradecanoic acid tetradecyl ester (C(28)H(56)O(2)) and methyl red (C(15)H(15)N(3)O(2)) mixture that has better permeability enabling its infiltration into wood and better thermochromic properties changing its colour at above 30 °C after about 0.5 min. Thicke...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group UK
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8377062/ https://www.ncbi.nlm.nih.gov/pubmed/34413331 http://dx.doi.org/10.1038/s41598-021-95274-2 |
_version_ | 1783740580344365056 |
---|---|
author | Zou, Weihua Li, Zimu Wang, Zhangheng Sun, Delin Zhang, Pingfang |
author_facet | Zou, Weihua Li, Zimu Wang, Zhangheng Sun, Delin Zhang, Pingfang |
author_sort | Zou, Weihua |
collection | PubMed |
description | The red thermochromic dye (R-TD) is the tetradecanoic acid tetradecyl ester (C(28)H(56)O(2)) and methyl red (C(15)H(15)N(3)O(2)) mixture that has better permeability enabling its infiltration into wood and better thermochromic properties changing its colour at above 30 °C after about 0.5 min. Thicker poplar-based thermochromic composite specimens (R-PTC, thickness: 5.0 mm) were prepared by filling the R-TD into pre-treated poplar veneer (thickness: 5.0 mm) thus allowing better penetration after pre-treatment. After R-TD infiltration, the R-PTC samples were covered by polypropylene wax for preventing R-TD from overflowing from R-PTC under the action of phase-change temperature. This R-PTC, whose colour can change from light-red to dark-red at 38 °C to 46 °C, can recover to light-red at below 38 °C after about 14 h, and the peak of colour change is at about 42 °C. R-PTC will be suitable for materials used in thermochromic furniture that can indicate the surface temperature to potential users, thus allowing assessment of likely scalded pain when used the furniture. |
format | Online Article Text |
id | pubmed-8377062 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2021 |
publisher | Nature Publishing Group UK |
record_format | MEDLINE/PubMed |
spelling | pubmed-83770622021-08-27 Poplar-based thermochromic composites that change colour at 38 °C to 46 °C Zou, Weihua Li, Zimu Wang, Zhangheng Sun, Delin Zhang, Pingfang Sci Rep Article The red thermochromic dye (R-TD) is the tetradecanoic acid tetradecyl ester (C(28)H(56)O(2)) and methyl red (C(15)H(15)N(3)O(2)) mixture that has better permeability enabling its infiltration into wood and better thermochromic properties changing its colour at above 30 °C after about 0.5 min. Thicker poplar-based thermochromic composite specimens (R-PTC, thickness: 5.0 mm) were prepared by filling the R-TD into pre-treated poplar veneer (thickness: 5.0 mm) thus allowing better penetration after pre-treatment. After R-TD infiltration, the R-PTC samples were covered by polypropylene wax for preventing R-TD from overflowing from R-PTC under the action of phase-change temperature. This R-PTC, whose colour can change from light-red to dark-red at 38 °C to 46 °C, can recover to light-red at below 38 °C after about 14 h, and the peak of colour change is at about 42 °C. R-PTC will be suitable for materials used in thermochromic furniture that can indicate the surface temperature to potential users, thus allowing assessment of likely scalded pain when used the furniture. Nature Publishing Group UK 2021-08-19 /pmc/articles/PMC8377062/ /pubmed/34413331 http://dx.doi.org/10.1038/s41598-021-95274-2 Text en © The Author(s) 2021 https://creativecommons.org/licenses/by/4.0/Open Access This article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons licence, and indicate if changes were made. The images or other third party material in this article are included in the article's Creative Commons licence, unless indicated otherwise in a credit line to the material. If material is not included in the article's Creative Commons licence and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this licence, visit http://creativecommons.org/licenses/by/4.0/ (https://creativecommons.org/licenses/by/4.0/) . |
spellingShingle | Article Zou, Weihua Li, Zimu Wang, Zhangheng Sun, Delin Zhang, Pingfang Poplar-based thermochromic composites that change colour at 38 °C to 46 °C |
title | Poplar-based thermochromic composites that change colour at 38 °C to 46 °C |
title_full | Poplar-based thermochromic composites that change colour at 38 °C to 46 °C |
title_fullStr | Poplar-based thermochromic composites that change colour at 38 °C to 46 °C |
title_full_unstemmed | Poplar-based thermochromic composites that change colour at 38 °C to 46 °C |
title_short | Poplar-based thermochromic composites that change colour at 38 °C to 46 °C |
title_sort | poplar-based thermochromic composites that change colour at 38 °c to 46 °c |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8377062/ https://www.ncbi.nlm.nih.gov/pubmed/34413331 http://dx.doi.org/10.1038/s41598-021-95274-2 |
work_keys_str_mv | AT zouweihua poplarbasedthermochromiccompositesthatchangecolourat38cto46c AT lizimu poplarbasedthermochromiccompositesthatchangecolourat38cto46c AT wangzhangheng poplarbasedthermochromiccompositesthatchangecolourat38cto46c AT sundelin poplarbasedthermochromiccompositesthatchangecolourat38cto46c AT zhangpingfang poplarbasedthermochromiccompositesthatchangecolourat38cto46c |