NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism

The NOx storage mechanism on BaTi(0.8)Cu(0.2)O(3) catalyst were studied using different techniques. The results obtained by XRD, ATR, TGA and XPS under NOx storage–regeneration conditions revealed that BaO generated on the catalyst by decomposition of Ba(2)TiO(4) plays a key role in the NOx storage...

Descripción completa

Detalles Bibliográficos
Autores principales: Albaladejo-Fuentes, Vicente, Sánchez-Adsuar, María-Salvadora, Anderson, James A., Illán-Gómez, María-José
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8401998/
https://www.ncbi.nlm.nih.gov/pubmed/34443963
http://dx.doi.org/10.3390/nano11082133
_version_ 1783745683494273024
author Albaladejo-Fuentes, Vicente
Sánchez-Adsuar, María-Salvadora
Anderson, James A.
Illán-Gómez, María-José
author_facet Albaladejo-Fuentes, Vicente
Sánchez-Adsuar, María-Salvadora
Anderson, James A.
Illán-Gómez, María-José
author_sort Albaladejo-Fuentes, Vicente
collection PubMed
description The NOx storage mechanism on BaTi(0.8)Cu(0.2)O(3) catalyst were studied using different techniques. The results obtained by XRD, ATR, TGA and XPS under NOx storage–regeneration conditions revealed that BaO generated on the catalyst by decomposition of Ba(2)TiO(4) plays a key role in the NOx storage process. In situ DRIFTS experiments under NO/O(2) and NO/N(2) show that nitrites and nitrates are formed on the perovskite during the NOx storage process. Thus, it seems that, as for model NSR catalysts, the NOx storage on BaTi(0.8)Cu(0.2)O(3) catalyst takes place by both “nitrite” and “nitrate” routes, with the main pathway being highly dependent on the temperature and the time on stream: (i) at T < 350 °C, NO adsorption leads to nitrites formation on the catalyst and (ii) at T > 350 °C, the catalyst activity for NO oxidation promotes NO(2) generation and the nitrate formation.
format Online
Article
Text
id pubmed-8401998
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-84019982021-08-29 NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism Albaladejo-Fuentes, Vicente Sánchez-Adsuar, María-Salvadora Anderson, James A. Illán-Gómez, María-José Nanomaterials (Basel) Article The NOx storage mechanism on BaTi(0.8)Cu(0.2)O(3) catalyst were studied using different techniques. The results obtained by XRD, ATR, TGA and XPS under NOx storage–regeneration conditions revealed that BaO generated on the catalyst by decomposition of Ba(2)TiO(4) plays a key role in the NOx storage process. In situ DRIFTS experiments under NO/O(2) and NO/N(2) show that nitrites and nitrates are formed on the perovskite during the NOx storage process. Thus, it seems that, as for model NSR catalysts, the NOx storage on BaTi(0.8)Cu(0.2)O(3) catalyst takes place by both “nitrite” and “nitrate” routes, with the main pathway being highly dependent on the temperature and the time on stream: (i) at T < 350 °C, NO adsorption leads to nitrites formation on the catalyst and (ii) at T > 350 °C, the catalyst activity for NO oxidation promotes NO(2) generation and the nitrate formation. MDPI 2021-08-21 /pmc/articles/PMC8401998/ /pubmed/34443963 http://dx.doi.org/10.3390/nano11082133 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Albaladejo-Fuentes, Vicente
Sánchez-Adsuar, María-Salvadora
Anderson, James A.
Illán-Gómez, María-José
NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism
title NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism
title_full NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism
title_fullStr NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism
title_full_unstemmed NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism
title_short NOx Storage on BaTi(0.8)Cu(0.2)O(3) Perovskite Catalysts: Addressing a Feasible Mechanism
title_sort nox storage on bati(0.8)cu(0.2)o(3) perovskite catalysts: addressing a feasible mechanism
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8401998/
https://www.ncbi.nlm.nih.gov/pubmed/34443963
http://dx.doi.org/10.3390/nano11082133
work_keys_str_mv AT albaladejofuentesvicente noxstorageonbati08cu02o3perovskitecatalystsaddressingafeasiblemechanism
AT sanchezadsuarmariasalvadora noxstorageonbati08cu02o3perovskitecatalystsaddressingafeasiblemechanism
AT andersonjamesa noxstorageonbati08cu02o3perovskitecatalystsaddressingafeasiblemechanism
AT illangomezmariajose noxstorageonbati08cu02o3perovskitecatalystsaddressingafeasiblemechanism