Unexpected High Ductility of Fe40Al Alloys at Room Temperature

Iron aluminium alloys, especially those sintered from elemental powders, suffer from low ductility. In this paper, an iron aluminium alloy (Fe40Al) produced by pressure-assisted induction sintering from elemental powders is shown and described. Samples produced by this method show an unexpectedly hi...