Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker

The purpose of this study was to evaluate the feasibility of using magnesium and sodium lignosulfonates (LS) in the production of particleboards, used pure and in mixtures with urea-formaldehyde (UF) resin. Polymeric 4,4′-diphenylmethane diisocyanate (pMDI) was used as a crosslinker. In order to eva...

Descripción completa

Detalles Bibliográficos
Autores principales: Bekhta, Pavlo, Noshchenko, Gregory, Réh, Roman, Kristak, Lubos, Sedliačik, Ján, Antov, Petar, Mirski, Radosław, Savov, Viktor
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8432716/
https://www.ncbi.nlm.nih.gov/pubmed/34500965
http://dx.doi.org/10.3390/ma14174875
_version_ 1783751223362453504
author Bekhta, Pavlo
Noshchenko, Gregory
Réh, Roman
Kristak, Lubos
Sedliačik, Ján
Antov, Petar
Mirski, Radosław
Savov, Viktor
author_facet Bekhta, Pavlo
Noshchenko, Gregory
Réh, Roman
Kristak, Lubos
Sedliačik, Ján
Antov, Petar
Mirski, Radosław
Savov, Viktor
author_sort Bekhta, Pavlo
collection PubMed
description The purpose of this study was to evaluate the feasibility of using magnesium and sodium lignosulfonates (LS) in the production of particleboards, used pure and in mixtures with urea-formaldehyde (UF) resin. Polymeric 4,4′-diphenylmethane diisocyanate (pMDI) was used as a crosslinker. In order to evaluate the effect of gradual replacement of UF by magnesium lignosulfonate (MgLS) or sodium lignosulfonate (NaLS) on the physical and mechanical properties, boards were manufactured in the laboratory with LS content varying from 0% to 100%. The effect of LS on the pH of lignosulfonate-urea-formaldehyde (LS-UF) adhesive compositions was also investigated. It was found that LS can be effectively used to adjust the pH of uncured and cured LS-UF formulations. Particleboards bonded with LS-UF adhesive formulations, comprising up to 30% LS, exhibited similar properties when compared to boards bonded with UF adhesive. The replacement of UF by both LS types substantially deteriorated the water absorption and thickness swelling of boards. In general, NaLS-UF-bonded boards had a lower formaldehyde content (FC) than MgLS-UF and UF-bonded boards as control. It was observed that in the process of manufacturing boards using LS adhesives, increasing the proportion of pMDI in the adhesive composition can significantly improve the mechanical properties of the boards. Overall, the boards fabricated using pure UF adhesives exhibited much better mechanical properties than boards bonded with LS adhesives. Markedly, the boards based on LS adhesives were characterised by a much lower FC than the UF-bonded boards. In the LS-bonded boards, the FC is lower by 91.1% and 56.9%, respectively, compared to the UF-bonded boards. The boards bonded with LS and pMDI had a close-to-zero FC and reached the super E0 emission class (≤1.5 mg/100 g) that allows for defining the laboratory-manufactured particleboards as eco-friendly composites.
format Online
Article
Text
id pubmed-8432716
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-84327162021-09-11 Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker Bekhta, Pavlo Noshchenko, Gregory Réh, Roman Kristak, Lubos Sedliačik, Ján Antov, Petar Mirski, Radosław Savov, Viktor Materials (Basel) Article The purpose of this study was to evaluate the feasibility of using magnesium and sodium lignosulfonates (LS) in the production of particleboards, used pure and in mixtures with urea-formaldehyde (UF) resin. Polymeric 4,4′-diphenylmethane diisocyanate (pMDI) was used as a crosslinker. In order to evaluate the effect of gradual replacement of UF by magnesium lignosulfonate (MgLS) or sodium lignosulfonate (NaLS) on the physical and mechanical properties, boards were manufactured in the laboratory with LS content varying from 0% to 100%. The effect of LS on the pH of lignosulfonate-urea-formaldehyde (LS-UF) adhesive compositions was also investigated. It was found that LS can be effectively used to adjust the pH of uncured and cured LS-UF formulations. Particleboards bonded with LS-UF adhesive formulations, comprising up to 30% LS, exhibited similar properties when compared to boards bonded with UF adhesive. The replacement of UF by both LS types substantially deteriorated the water absorption and thickness swelling of boards. In general, NaLS-UF-bonded boards had a lower formaldehyde content (FC) than MgLS-UF and UF-bonded boards as control. It was observed that in the process of manufacturing boards using LS adhesives, increasing the proportion of pMDI in the adhesive composition can significantly improve the mechanical properties of the boards. Overall, the boards fabricated using pure UF adhesives exhibited much better mechanical properties than boards bonded with LS adhesives. Markedly, the boards based on LS adhesives were characterised by a much lower FC than the UF-bonded boards. In the LS-bonded boards, the FC is lower by 91.1% and 56.9%, respectively, compared to the UF-bonded boards. The boards bonded with LS and pMDI had a close-to-zero FC and reached the super E0 emission class (≤1.5 mg/100 g) that allows for defining the laboratory-manufactured particleboards as eco-friendly composites. MDPI 2021-08-27 /pmc/articles/PMC8432716/ /pubmed/34500965 http://dx.doi.org/10.3390/ma14174875 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Bekhta, Pavlo
Noshchenko, Gregory
Réh, Roman
Kristak, Lubos
Sedliačik, Ján
Antov, Petar
Mirski, Radosław
Savov, Viktor
Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker
title Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker
title_full Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker
title_fullStr Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker
title_full_unstemmed Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker
title_short Properties of Eco-Friendly Particleboards Bonded with Lignosulfonate-Urea-Formaldehyde Adhesives and pMDI as a Crosslinker
title_sort properties of eco-friendly particleboards bonded with lignosulfonate-urea-formaldehyde adhesives and pmdi as a crosslinker
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8432716/
https://www.ncbi.nlm.nih.gov/pubmed/34500965
http://dx.doi.org/10.3390/ma14174875
work_keys_str_mv AT bekhtapavlo propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker
AT noshchenkogregory propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker
AT rehroman propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker
AT kristaklubos propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker
AT sedliacikjan propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker
AT antovpetar propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker
AT mirskiradosław propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker
AT savovviktor propertiesofecofriendlyparticleboardsbondedwithlignosulfonateureaformaldehydeadhesivesandpmdiasacrosslinker