Cargando…

Influence of Solution Treatment Time on Precipitation Behavior and Mechanical Properties of Mg-2.0Nd-2.0Sm-0.4Zn-0.4Zr Alloy

The effect of solution treatment time on the microstructure and mechanical properties of aged the Mg-2.0Nd-2.0Sm-0.4Zn-0.4Zr (wt.%) alloy were investigated to give full play to the performance of the alloy. As the solution treatment time increased from 2 h to 12 h at 788 K, the grain size of the sol...

Descripción completa

Detalles Bibliográficos
Autores principales: Ma, Tao, Zhao, Sicong, Wang, Liping, Wang, Zhiwei, Guo, Erjun, Feng, Yicheng, Li, Jingfang
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8433664/
https://www.ncbi.nlm.nih.gov/pubmed/34501125
http://dx.doi.org/10.3390/ma14175037
Descripción
Sumario:The effect of solution treatment time on the microstructure and mechanical properties of aged the Mg-2.0Nd-2.0Sm-0.4Zn-0.4Zr (wt.%) alloy were investigated to give full play to the performance of the alloy. As the solution treatment time increased from 2 h to 12 h at 788 K, the grain size of the solution-treated alloy significantly increased, and the network-like β-Mg(12)(Nd, Sm, Zn) phase gradually dissolved into the α-Mg matrix. It should be noted that no obvious residual β phase can be observed when the solution treatment time was more than 8 h. After the solution-treated alloy was further aged at 473 K for 18 h, a large number of nanoscale precipitates were observed in the α-Mg matrix. The solution treatment time was 2 h, the α-Mg matrix mainly consisted of spherical-shaped and basal plate-shaped precipitates. Upon the increase of solution treatment time to 8 h, the key strengthening phases transformed from spherical-shaped precipitates and basal plate-shaped precipitates to prismatic plate-shaped β′ precipitates. The orientation relationship between β′ precipitates and α-Mg matrix was ([Formula: see text] 10)(β)(′) // (1 [Formula: see text] 00)(α) and [112](β)(′) // the [22 [Formula: see text] 3](α). Further increasing of solution treatment time from 8 h to 12 h, the key strengthening phases mainly were still β′ precipitates. The solution treatment of aged alloy was carried out at 788 K for 8 h, which achieved optimal ultimate tensile strength (UTS) of 261 ± 4.1 MPa, yield strength (YS) of 154 ± 1.5 MPa, and elongation of 5.8 ± 0.1%, respectively.