Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture

Crystalline admixtures embedded in concrete may react in the presence of water and generate thin crystals able to fill pores, capillaries and micro-cracks. Once the concrete has dried, the crystalline chemicals sit dormant until another dose of water starts the crystallization again. The research ai...

Descripción completa

Detalles Bibliográficos
Autores principales: Mircea, Calin, Toader, Tudor-Panfil, Hegyi, Andreea, Ionescu, Brăduț-Alexandru, Mircea, Andreea
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8434591/
https://www.ncbi.nlm.nih.gov/pubmed/34501041
http://dx.doi.org/10.3390/ma14174951
_version_ 1783751636223524864
author Mircea, Calin
Toader, Tudor-Panfil
Hegyi, Andreea
Ionescu, Brăduț-Alexandru
Mircea, Andreea
author_facet Mircea, Calin
Toader, Tudor-Panfil
Hegyi, Andreea
Ionescu, Brăduț-Alexandru
Mircea, Andreea
author_sort Mircea, Calin
collection PubMed
description Crystalline admixtures embedded in concrete may react in the presence of water and generate thin crystals able to fill pores, capillaries and micro-cracks. Once the concrete has dried, the crystalline chemicals sit dormant until another dose of water starts the crystallization again. The research aims to analyses the early age self-sealing effect of a crystalline admixture at a dosage rate of 1–3% of the cement mass. Specimens made with two types of gravel were pre-loaded with three-point bending to up to 90% of the ultimate capacity, and conditioned through wet–dry cycles. Micro-crack closure was measured with a microscope after pre-loading, and after 1 day, 4 days, 8 days, 14 days and 20 days of wet–dry exposure. The results show that an admixture content of 3% achieves the best early self-sealing performance. These results are also confirmed by probabilistic analyses, which also emphasize the self-sealing potential of lower ICW contents.
format Online
Article
Text
id pubmed-8434591
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-84345912021-09-12 Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture Mircea, Calin Toader, Tudor-Panfil Hegyi, Andreea Ionescu, Brăduț-Alexandru Mircea, Andreea Materials (Basel) Article Crystalline admixtures embedded in concrete may react in the presence of water and generate thin crystals able to fill pores, capillaries and micro-cracks. Once the concrete has dried, the crystalline chemicals sit dormant until another dose of water starts the crystallization again. The research aims to analyses the early age self-sealing effect of a crystalline admixture at a dosage rate of 1–3% of the cement mass. Specimens made with two types of gravel were pre-loaded with three-point bending to up to 90% of the ultimate capacity, and conditioned through wet–dry cycles. Micro-crack closure was measured with a microscope after pre-loading, and after 1 day, 4 days, 8 days, 14 days and 20 days of wet–dry exposure. The results show that an admixture content of 3% achieves the best early self-sealing performance. These results are also confirmed by probabilistic analyses, which also emphasize the self-sealing potential of lower ICW contents. MDPI 2021-08-30 /pmc/articles/PMC8434591/ /pubmed/34501041 http://dx.doi.org/10.3390/ma14174951 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Mircea, Calin
Toader, Tudor-Panfil
Hegyi, Andreea
Ionescu, Brăduț-Alexandru
Mircea, Andreea
Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture
title Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture
title_full Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture
title_fullStr Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture
title_full_unstemmed Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture
title_short Early Age Sealing Capacity of Structural Mortar with Integral Crystalline Waterproofing Admixture
title_sort early age sealing capacity of structural mortar with integral crystalline waterproofing admixture
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8434591/
https://www.ncbi.nlm.nih.gov/pubmed/34501041
http://dx.doi.org/10.3390/ma14174951
work_keys_str_mv AT mirceacalin earlyagesealingcapacityofstructuralmortarwithintegralcrystallinewaterproofingadmixture
AT toadertudorpanfil earlyagesealingcapacityofstructuralmortarwithintegralcrystallinewaterproofingadmixture
AT hegyiandreea earlyagesealingcapacityofstructuralmortarwithintegralcrystallinewaterproofingadmixture
AT ionescubradutalexandru earlyagesealingcapacityofstructuralmortarwithintegralcrystallinewaterproofingadmixture
AT mirceaandreea earlyagesealingcapacityofstructuralmortarwithintegralcrystallinewaterproofingadmixture