Initiation and Suppression of Crack Propagation during Magnesium Alloy Rolling
The conventional rolling of magnesium alloy with a single pass and large reduction will cause severe edge cracking. The sheet without cracks can be achieved by limited width rolling. The microstructure evolution of the sheet with cracks after conventional rolling and the sheet without cracks after l...
Autores principales: | Tian, Jing, Shi, Quan-Xin, Meng, Li-Xin, Deng, Jia-Fei, Liang, Wei, Ma, Jin-Yao |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8467149/ https://www.ncbi.nlm.nih.gov/pubmed/34576437 http://dx.doi.org/10.3390/ma14185217 |
Ejemplares similares
-
Crack Propagation Analysis of Compression Loaded Rolling Elements
por: Dlhý, Pavol, et al.
Publicado: (2021) -
Effect of Temperature Field and Stress Field of Different Crack Behavior on Twins and Dislocations under Mg Alloy Rolling
por: Tian, Jing, et al.
Publicado: (2021) -
Enhanced Formability of Magnesium Alloy Rolled Plates by [Formula: see text] Tensile Twinning and Recrystallization
por: Deng, Jiafei, et al.
Publicado: (2022) -
Quasi-In-Situ Analysis of As-Rolled Microstructure of Magnesium Alloys during Annealing and Subsequent Plastic Deformation
por: Deng, Jiafei, et al.
Publicado: (2022) -
The Effect of ECAP Temperature on the Microstructure and Properties of a Rolled Rare Earth Magnesium Alloy
por: Tan, Yun, et al.
Publicado: (2019)