Complex metallic alloys (CMAs) are materials composed of structurally complex intermetallic phases (SCIPs). The SCIPs consist of large unit cells containing hundreds or even thousands of atoms. Well-defined atomic clusters are found in their structure, typically of icosahedral point group symmetry....

Descripción completa

Detalles Bibliográficos
Autores principales: Ďuriška, Libor, Černičková, Ivona, Priputen, Pavol, Palcut, Marián
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8467597/
https://www.ncbi.nlm.nih.gov/pubmed/34576643
http://dx.doi.org/10.3390/ma14185418
_version_ 1784573438489264128
author Ďuriška, Libor
Černičková, Ivona
Priputen, Pavol
Palcut, Marián
author_facet Ďuriška, Libor
Černičková, Ivona
Priputen, Pavol
Palcut, Marián
author_sort Ďuriška, Libor
collection PubMed
description Complex metallic alloys (CMAs) are materials composed of structurally complex intermetallic phases (SCIPs). The SCIPs consist of large unit cells containing hundreds or even thousands of atoms. Well-defined atomic clusters are found in their structure, typically of icosahedral point group symmetry. In SCIPs, a long-range order is observed. Aluminum-based CMAs contain approximately 70 at.% Al. In this paper, the corrosion behavior of bulk Al-based CMAs is reviewed. The Al–TM alloys (TM = transition metal) have been sorted according to their chemical composition. The alloys tend to passivate because of high Al concentration. The Al–Cr alloys, for example, can form protective passive layers of considerable thickness in different electrolytes. In halide-containing solutions, however, the alloys are prone to pitting corrosion. The electrochemical activity of aluminum-transition metal SCIPs is primarily determined by electrode potential of the alloying element(s). Galvanic microcells form between different SCIPs which may further accelerate the localized corrosion attack. The electrochemical nobility of individual SCIPs increases with increasing concentration of noble elements. The SCIPs with electrochemically active elements tend to dissolve in contact with nobler particles. The SCIPs with noble metals are prone to selective de-alloying (de–aluminification) and their electrochemical activity may change over time as a result of de-alloying. The metal composition of the SCIPs has a primary influence on their corrosion properties. The structural complexity is secondary and becomes important when phases with similar chemical composition, but different crystal structure, come into close physical contact.
format Online
Article
Text
id pubmed-8467597
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-84675972021-09-27 Aqueous Corrosion of Aluminum-Transition Metal Alloys Composed of Structurally Complex Phases: A Review Ďuriška, Libor Černičková, Ivona Priputen, Pavol Palcut, Marián Materials (Basel) Review Complex metallic alloys (CMAs) are materials composed of structurally complex intermetallic phases (SCIPs). The SCIPs consist of large unit cells containing hundreds or even thousands of atoms. Well-defined atomic clusters are found in their structure, typically of icosahedral point group symmetry. In SCIPs, a long-range order is observed. Aluminum-based CMAs contain approximately 70 at.% Al. In this paper, the corrosion behavior of bulk Al-based CMAs is reviewed. The Al–TM alloys (TM = transition metal) have been sorted according to their chemical composition. The alloys tend to passivate because of high Al concentration. The Al–Cr alloys, for example, can form protective passive layers of considerable thickness in different electrolytes. In halide-containing solutions, however, the alloys are prone to pitting corrosion. The electrochemical activity of aluminum-transition metal SCIPs is primarily determined by electrode potential of the alloying element(s). Galvanic microcells form between different SCIPs which may further accelerate the localized corrosion attack. The electrochemical nobility of individual SCIPs increases with increasing concentration of noble elements. The SCIPs with electrochemically active elements tend to dissolve in contact with nobler particles. The SCIPs with noble metals are prone to selective de-alloying (de–aluminification) and their electrochemical activity may change over time as a result of de-alloying. The metal composition of the SCIPs has a primary influence on their corrosion properties. The structural complexity is secondary and becomes important when phases with similar chemical composition, but different crystal structure, come into close physical contact. MDPI 2021-09-19 /pmc/articles/PMC8467597/ /pubmed/34576643 http://dx.doi.org/10.3390/ma14185418 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Review
Ďuriška, Libor
Černičková, Ivona
Priputen, Pavol
Palcut, Marián
Aqueous Corrosion of Aluminum-Transition Metal Alloys Composed of Structurally Complex Phases: A Review
title Aqueous Corrosion of Aluminum-Transition Metal Alloys Composed of Structurally Complex Phases: A Review
title_full Aqueous Corrosion of Aluminum-Transition Metal Alloys Composed of Structurally Complex Phases: A Review
title_fullStr Aqueous Corrosion of Aluminum-Transition Metal Alloys Composed of Structurally Complex Phases: A Review
title_full_unstemmed Aqueous Corrosion of Aluminum-Transition Metal Alloys Composed of Structurally Complex Phases: A Review
title_short Aqueous Corrosion of Aluminum-Transition Metal Alloys Composed of Structurally Complex Phases: A Review
title_sort aqueous corrosion of aluminum-transition metal alloys composed of structurally complex phases: a review
topic Review
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8467597/
https://www.ncbi.nlm.nih.gov/pubmed/34576643
http://dx.doi.org/10.3390/ma14185418
work_keys_str_mv AT duriskalibor aqueouscorrosionofaluminumtransitionmetalalloyscomposedofstructurallycomplexphasesareview
AT cernickovaivona aqueouscorrosionofaluminumtransitionmetalalloyscomposedofstructurallycomplexphasesareview
AT priputenpavol aqueouscorrosionofaluminumtransitionmetalalloyscomposedofstructurallycomplexphasesareview
AT palcutmarian aqueouscorrosionofaluminumtransitionmetalalloyscomposedofstructurallycomplexphasesareview