Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint

Weld and base metals require hot or cold working during the steel equipment manufacturing process. As a result, the components should be subjected to a normalizing heat treatment in order to recover their mechanical properties. In this study, the submerged-arc welding of the high strength low alloy...

Descripción completa

Detalles Bibliográficos
Autores principales: Tian, Songya, Xu, Fan, Zhang, Genyuan, Saifan, Adnan, Saleh, Bassiouny, Li, Xiaobo
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8470230/
https://www.ncbi.nlm.nih.gov/pubmed/34576560
http://dx.doi.org/10.3390/ma14185336
_version_ 1784574145592295424
author Tian, Songya
Xu, Fan
Zhang, Genyuan
Saifan, Adnan
Saleh, Bassiouny
Li, Xiaobo
author_facet Tian, Songya
Xu, Fan
Zhang, Genyuan
Saifan, Adnan
Saleh, Bassiouny
Li, Xiaobo
author_sort Tian, Songya
collection PubMed
description Weld and base metals require hot or cold working during the steel equipment manufacturing process. As a result, the components should be subjected to a normalizing heat treatment in order to recover their mechanical properties. In this study, the submerged-arc welding of the high strength low alloy (HSLA) thick steel plate(13MnNiMoR) is adapted for the vessel head under the normalizing and tempering heat treatment. The findings showed that the material toughness decreases after heating to simulate a vessel head forming process. The stamping process is carried out under the conditions of 980 °C for one hour, normalizing at 920 °C for 1 h and tempering between 600–660 °C for 2 h, respectively. The martensite-austenite (M-A) constituent is distributed in granular bainite and the boundary of austenite in island constituent. Therefore, it was deemed to be the most detrimental to Charpy-V impact toughness. Between normalizing and tempering, intercritical normalizing at 740 °C was added. As a result of the ferrite with fine particles M-A constituent, the toughness increases significantly.
format Online
Article
Text
id pubmed-8470230
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-84702302021-09-27 Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint Tian, Songya Xu, Fan Zhang, Genyuan Saifan, Adnan Saleh, Bassiouny Li, Xiaobo Materials (Basel) Article Weld and base metals require hot or cold working during the steel equipment manufacturing process. As a result, the components should be subjected to a normalizing heat treatment in order to recover their mechanical properties. In this study, the submerged-arc welding of the high strength low alloy (HSLA) thick steel plate(13MnNiMoR) is adapted for the vessel head under the normalizing and tempering heat treatment. The findings showed that the material toughness decreases after heating to simulate a vessel head forming process. The stamping process is carried out under the conditions of 980 °C for one hour, normalizing at 920 °C for 1 h and tempering between 600–660 °C for 2 h, respectively. The martensite-austenite (M-A) constituent is distributed in granular bainite and the boundary of austenite in island constituent. Therefore, it was deemed to be the most detrimental to Charpy-V impact toughness. Between normalizing and tempering, intercritical normalizing at 740 °C was added. As a result of the ferrite with fine particles M-A constituent, the toughness increases significantly. MDPI 2021-09-16 /pmc/articles/PMC8470230/ /pubmed/34576560 http://dx.doi.org/10.3390/ma14185336 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Tian, Songya
Xu, Fan
Zhang, Genyuan
Saifan, Adnan
Saleh, Bassiouny
Li, Xiaobo
Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint
title Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint
title_full Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint
title_fullStr Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint
title_full_unstemmed Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint
title_short Influence of Post-Weld Heat Treatment on Microstructure and Toughness Properties of 13MnNiMoR High Strength Low Alloy Steel Weld Joint
title_sort influence of post-weld heat treatment on microstructure and toughness properties of 13mnnimor high strength low alloy steel weld joint
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8470230/
https://www.ncbi.nlm.nih.gov/pubmed/34576560
http://dx.doi.org/10.3390/ma14185336
work_keys_str_mv AT tiansongya influenceofpostweldheattreatmentonmicrostructureandtoughnesspropertiesof13mnnimorhighstrengthlowalloysteelweldjoint
AT xufan influenceofpostweldheattreatmentonmicrostructureandtoughnesspropertiesof13mnnimorhighstrengthlowalloysteelweldjoint
AT zhanggenyuan influenceofpostweldheattreatmentonmicrostructureandtoughnesspropertiesof13mnnimorhighstrengthlowalloysteelweldjoint
AT saifanadnan influenceofpostweldheattreatmentonmicrostructureandtoughnesspropertiesof13mnnimorhighstrengthlowalloysteelweldjoint
AT salehbassiouny influenceofpostweldheattreatmentonmicrostructureandtoughnesspropertiesof13mnnimorhighstrengthlowalloysteelweldjoint
AT lixiaobo influenceofpostweldheattreatmentonmicrostructureandtoughnesspropertiesof13mnnimorhighstrengthlowalloysteelweldjoint