Synthesis of Tailored Perfluoro Unsaturated Monomers for Potential Applications in Proton Exchange Membrane Preparation

The aim of the present work is the synthesis and characterization of new perfluorinated monomers bearing, similarly to Nafion(®), acidic groups for proton transport for potential and future applications in proton exchange membrane (PEM) fuel cells. To this end, we focused our attention on the synthe...

Descripción completa

Detalles Bibliográficos
Autores principales: Monopoli, Antonio, Casiello, Michele, Cotugno, Pietro, Milella, Antonella, Palumbo, Fabio, Fracassi, Francesco, Nacci, Angelo
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8470954/
https://www.ncbi.nlm.nih.gov/pubmed/34577063
http://dx.doi.org/10.3390/molecules26185592
Descripción
Sumario:The aim of the present work is the synthesis and characterization of new perfluorinated monomers bearing, similarly to Nafion(®), acidic groups for proton transport for potential and future applications in proton exchange membrane (PEM) fuel cells. To this end, we focused our attention on the synthesis of various molecules with (i) sufficient volatility to be used in vacuum polymerization techniques (e.g., PECVD)), (ii) sulfonic, phosphonic, or carboxylic acid functionalities for proton transport capacity of the resulting membrane, (iii) both aliphatic and aromatic perfluorinated tags to diversify the membrane polarity with respect to Nafion(®), and (iv) a double bond to facilitate the polymerization under vacuum giving a preferential way for the chain growth of the polymer. A retrosynthetic approach persuaded us to attempt three main synthetic strategies: (a) organometallic Heck-type cross-coupling, (b) nucleophilic displacement, and (c) Wittig–Horner reaction (carbanion approach). Preliminary results on the plasma deposition of a polymeric film are also presented. The variation of plasma conditions allowed us to point out that the film prepared in the mildest settings (20 W) shows the maximum monomer retention in its structure. In this condition, plasma polymerization likely occurs mainly by rupture of the π bond in the monomer molecule.