Cavitation Erosion of Ni-Based Superalloys Manufactured by Forging and Additive Manufacturing

Inconel pipes that transport cryogenic fluids in rocket engines manufactured by additive manufacturing (AM) were eroded by cavitation. The AM method selective laser melting (SLM) was used to manufacture at lower cost, but had seemingly lower erosion resistance. The cavitation erosion properties of I...