Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route
In the present work, we investigated the possibility of introducing fine and densely distributed α-Al(MnFe)Si dispersoids into the microstructure of extruded Al-Mg-Si-Mn AA6082 alloys containing 0.5 and 1 wt % Mn through tailoring the processing route as well as their effects on room- and elevated-t...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8509739/ https://www.ncbi.nlm.nih.gov/pubmed/34639888 http://dx.doi.org/10.3390/ma14195489 |
_version_ | 1784582415855910912 |
---|---|
author | Rakhmonov, Jovid Liu, Kun Rometsch, Paul Parson, Nick Chen, X.-Grant |
author_facet | Rakhmonov, Jovid Liu, Kun Rometsch, Paul Parson, Nick Chen, X.-Grant |
author_sort | Rakhmonov, Jovid |
collection | PubMed |
description | In the present work, we investigated the possibility of introducing fine and densely distributed α-Al(MnFe)Si dispersoids into the microstructure of extruded Al-Mg-Si-Mn AA6082 alloys containing 0.5 and 1 wt % Mn through tailoring the processing route as well as their effects on room- and elevated-temperature strength and creep resistance. The results show that the fine dispersoids formed during low-temperature homogenization experienced less coarsening when subsequently extruded at 350 °C than when subjected to a more typical high-temperature extrusion at 500 °C. After aging, a significant strengthening effect was produced by β″ precipitates in all conditions studied. Fine dispersoids offered complimentary strengthening, further enhancing the room-temperature compressive yield strength by up to 72–77 MPa (≈28%) relative to the alloy with coarse dispersoids. During thermal exposure at 300 °C for 100 h, β″ precipitates transformed into undesirable β-Mg(2)Si, while thermally stable dispersoids provided the predominant elevated-temperature strengthening effect. Compared to the base case with coarse dispersoids, fine and densely distributed dispersoids with the new processing route more than doubled the yield strength at 300 °C. In addition, finer dispersoids obtained by extrusion at 350 °C improved the yield strength at 300 °C by 17% compared to that at 500 °C. The creep resistance at 300 °C was greatly improved by an order of magnitude from the coarse dispersoid condition to one containing fine and densely distributed dispersoids, highlighting the high efficacy of the new processing route in enhancing the elevated-temperature properties of extruded Al-Mg-Si-Mn alloys. |
format | Online Article Text |
id | pubmed-8509739 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2021 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-85097392021-10-13 Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route Rakhmonov, Jovid Liu, Kun Rometsch, Paul Parson, Nick Chen, X.-Grant Materials (Basel) Article In the present work, we investigated the possibility of introducing fine and densely distributed α-Al(MnFe)Si dispersoids into the microstructure of extruded Al-Mg-Si-Mn AA6082 alloys containing 0.5 and 1 wt % Mn through tailoring the processing route as well as their effects on room- and elevated-temperature strength and creep resistance. The results show that the fine dispersoids formed during low-temperature homogenization experienced less coarsening when subsequently extruded at 350 °C than when subjected to a more typical high-temperature extrusion at 500 °C. After aging, a significant strengthening effect was produced by β″ precipitates in all conditions studied. Fine dispersoids offered complimentary strengthening, further enhancing the room-temperature compressive yield strength by up to 72–77 MPa (≈28%) relative to the alloy with coarse dispersoids. During thermal exposure at 300 °C for 100 h, β″ precipitates transformed into undesirable β-Mg(2)Si, while thermally stable dispersoids provided the predominant elevated-temperature strengthening effect. Compared to the base case with coarse dispersoids, fine and densely distributed dispersoids with the new processing route more than doubled the yield strength at 300 °C. In addition, finer dispersoids obtained by extrusion at 350 °C improved the yield strength at 300 °C by 17% compared to that at 500 °C. The creep resistance at 300 °C was greatly improved by an order of magnitude from the coarse dispersoid condition to one containing fine and densely distributed dispersoids, highlighting the high efficacy of the new processing route in enhancing the elevated-temperature properties of extruded Al-Mg-Si-Mn alloys. MDPI 2021-09-23 /pmc/articles/PMC8509739/ /pubmed/34639888 http://dx.doi.org/10.3390/ma14195489 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Rakhmonov, Jovid Liu, Kun Rometsch, Paul Parson, Nick Chen, X.-Grant Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route |
title | Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route |
title_full | Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route |
title_fullStr | Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route |
title_full_unstemmed | Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route |
title_short | Enhanced Elevated-Temperature Strength and Creep Resistance of Dispersion-Strengthened Al-Mg-Si-Mn AA6082 Alloys through Modified Processing Route |
title_sort | enhanced elevated-temperature strength and creep resistance of dispersion-strengthened al-mg-si-mn aa6082 alloys through modified processing route |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8509739/ https://www.ncbi.nlm.nih.gov/pubmed/34639888 http://dx.doi.org/10.3390/ma14195489 |
work_keys_str_mv | AT rakhmonovjovid enhancedelevatedtemperaturestrengthandcreepresistanceofdispersionstrengthenedalmgsimnaa6082alloysthroughmodifiedprocessingroute AT liukun enhancedelevatedtemperaturestrengthandcreepresistanceofdispersionstrengthenedalmgsimnaa6082alloysthroughmodifiedprocessingroute AT rometschpaul enhancedelevatedtemperaturestrengthandcreepresistanceofdispersionstrengthenedalmgsimnaa6082alloysthroughmodifiedprocessingroute AT parsonnick enhancedelevatedtemperaturestrengthandcreepresistanceofdispersionstrengthenedalmgsimnaa6082alloysthroughmodifiedprocessingroute AT chenxgrant enhancedelevatedtemperaturestrengthandcreepresistanceofdispersionstrengthenedalmgsimnaa6082alloysthroughmodifiedprocessingroute |