Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines

Water pipe surface deterioration is the result of continuous electrochemical reactions attacking the surface due to the interaction of the pipe surface with environments through the time function. The study presents corrosion characterization at the surface and sub-surface of damaged ductile iron pi...

Descripción completa

Detalles Bibliográficos
Autores principales: Yeshanew, Dessalegn Ahmed, Jiru, Moera Gutu, Ahmed, Gulam Mohammed Sayeed, Badruddin, Irfan Anjum, Soudagar, Manzoore Elahi M., Kamangar, Sarfaraz, Tolcha, Mesay Alemu
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8510394/
https://www.ncbi.nlm.nih.gov/pubmed/34640274
http://dx.doi.org/10.3390/ma14195877
_version_ 1784582561331150848
author Yeshanew, Dessalegn Ahmed
Jiru, Moera Gutu
Ahmed, Gulam Mohammed Sayeed
Badruddin, Irfan Anjum
Soudagar, Manzoore Elahi M.
Kamangar, Sarfaraz
Tolcha, Mesay Alemu
author_facet Yeshanew, Dessalegn Ahmed
Jiru, Moera Gutu
Ahmed, Gulam Mohammed Sayeed
Badruddin, Irfan Anjum
Soudagar, Manzoore Elahi M.
Kamangar, Sarfaraz
Tolcha, Mesay Alemu
author_sort Yeshanew, Dessalegn Ahmed
collection PubMed
description Water pipe surface deterioration is the result of continuous electrochemical reactions attacking the surface due to the interaction of the pipe surface with environments through the time function. The study presents corrosion characterization at the surface and sub-surface of damaged ductile iron pipe (DIP) and galvanized steel (GS) pipes which served for more than 40 and 20 years, respectively. The samples were obtained from Addis Ababa city water distribution system for the analysis of corrosion morphology patterns at different surface layers. Mountains 8.2 surface analysis software was utilized based on the ISO 25178-2 watershed segmentation method to investigate corrosion features of damaged pipe surface and to evaluate maximum pit depth, area, and volume in-situ condition. Based on the analysis maximum values of pit depth, area and volume were 380 [Formula: see text] m, 4000 [Formula: see text] m(2), and 200,000 [Formula: see text] m(3), respectively, after 25% loss of the original 8 mm thickness of DIP. Similarly, the pit depth of the GS pipe was 390 [Formula: see text] whereas the maximum pit area and volume are 4000 [Formula: see text] m(2) and 16,000 [Formula: see text] m(3), respectively. In addition, characterizations of new pipes were evaluated to study microstructures by using an optical microscope (OM), and a scanning electron microscope (SEM) was used to analyze corrosion morphologies. Based on the SEM analysis, cracks were observed at the sub-surface layer of the pipes. The results show that uniform corrosion attacked the external pipe surface whereas pitting corrosion damaged the subsurface of pipes. The output of this study will be utilized by water suppliers and industries to investigate corrosion phenomena at any damage stage.
format Online
Article
Text
id pubmed-8510394
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-85103942021-10-13 Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines Yeshanew, Dessalegn Ahmed Jiru, Moera Gutu Ahmed, Gulam Mohammed Sayeed Badruddin, Irfan Anjum Soudagar, Manzoore Elahi M. Kamangar, Sarfaraz Tolcha, Mesay Alemu Materials (Basel) Article Water pipe surface deterioration is the result of continuous electrochemical reactions attacking the surface due to the interaction of the pipe surface with environments through the time function. The study presents corrosion characterization at the surface and sub-surface of damaged ductile iron pipe (DIP) and galvanized steel (GS) pipes which served for more than 40 and 20 years, respectively. The samples were obtained from Addis Ababa city water distribution system for the analysis of corrosion morphology patterns at different surface layers. Mountains 8.2 surface analysis software was utilized based on the ISO 25178-2 watershed segmentation method to investigate corrosion features of damaged pipe surface and to evaluate maximum pit depth, area, and volume in-situ condition. Based on the analysis maximum values of pit depth, area and volume were 380 [Formula: see text] m, 4000 [Formula: see text] m(2), and 200,000 [Formula: see text] m(3), respectively, after 25% loss of the original 8 mm thickness of DIP. Similarly, the pit depth of the GS pipe was 390 [Formula: see text] whereas the maximum pit area and volume are 4000 [Formula: see text] m(2) and 16,000 [Formula: see text] m(3), respectively. In addition, characterizations of new pipes were evaluated to study microstructures by using an optical microscope (OM), and a scanning electron microscope (SEM) was used to analyze corrosion morphologies. Based on the SEM analysis, cracks were observed at the sub-surface layer of the pipes. The results show that uniform corrosion attacked the external pipe surface whereas pitting corrosion damaged the subsurface of pipes. The output of this study will be utilized by water suppliers and industries to investigate corrosion phenomena at any damage stage. MDPI 2021-10-07 /pmc/articles/PMC8510394/ /pubmed/34640274 http://dx.doi.org/10.3390/ma14195877 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Yeshanew, Dessalegn Ahmed
Jiru, Moera Gutu
Ahmed, Gulam Mohammed Sayeed
Badruddin, Irfan Anjum
Soudagar, Manzoore Elahi M.
Kamangar, Sarfaraz
Tolcha, Mesay Alemu
Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines
title Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines
title_full Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines
title_fullStr Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines
title_full_unstemmed Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines
title_short Corrosion Characterization at Surface and Subsurface of Iron-Based Buried Water Pipelines
title_sort corrosion characterization at surface and subsurface of iron-based buried water pipelines
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8510394/
https://www.ncbi.nlm.nih.gov/pubmed/34640274
http://dx.doi.org/10.3390/ma14195877
work_keys_str_mv AT yeshanewdessalegnahmed corrosioncharacterizationatsurfaceandsubsurfaceofironbasedburiedwaterpipelines
AT jirumoeragutu corrosioncharacterizationatsurfaceandsubsurfaceofironbasedburiedwaterpipelines
AT ahmedgulammohammedsayeed corrosioncharacterizationatsurfaceandsubsurfaceofironbasedburiedwaterpipelines
AT badruddinirfananjum corrosioncharacterizationatsurfaceandsubsurfaceofironbasedburiedwaterpipelines
AT soudagarmanzooreelahim corrosioncharacterizationatsurfaceandsubsurfaceofironbasedburiedwaterpipelines
AT kamangarsarfaraz corrosioncharacterizationatsurfaceandsubsurfaceofironbasedburiedwaterpipelines
AT tolchamesayalemu corrosioncharacterizationatsurfaceandsubsurfaceofironbasedburiedwaterpipelines