Comparative Evaluation of Marginal Integrity of Three Esthetic Restorative Materials – An In-vitro Study
CONTEXT: Microleakage is the major cause for the failure of dental restorations, especially in Class V cavities, as margins of such restorations are generally located in dentin or cementum. Microleakage evaluation is necessary as a means of evaluation of the marginal integrity of restorative materia...
Autores principales: | Singh, Sukhdeep, Goel, Dhirja, Awasthi, Neha, Khandelwal, Deepak, Sharma, Aakansha, Patil, Seema |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Wolters Kluwer - Medknow
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8525820/ https://www.ncbi.nlm.nih.gov/pubmed/34759680 http://dx.doi.org/10.4103/ccd.ccd_318_20 |
Ejemplares similares
-
Restoring Esthetics after Anterior Tooth Loss for a Five-Year-Old Child: Natural Tooth Pontic Fiber Reinforced Prosthesis
por: Goel, Dhirja, et al.
Publicado: (2013) -
In vitro evaluation of the marginal and internal discrepancies of
different esthetic restorations
por: SAKRANA, Amal Abdelsamad
Publicado: (2013) -
The effect of red wine on colour stability of three different types of esthetic restorative materials: An in vitro study
por: Chakravarthy, Yadav, et al.
Publicado: (2018) -
Comparison of Shear Bond Strength of Three Commercially Available Esthetic Restorative Composite Materials: An In Vitro Study
por: Preethy, Neethu A, et al.
Publicado: (2020) -
Comparative Evaluation of the Surface Hardness of Different Esthetic Restorative Materials: An In Vitro Study
por: Samuel, Anoop, et al.
Publicado: (2020)