Abrasive Wear of High-Carbon Low-Alloyed Austenite Steel: Microhardness, Microstructure and X-ray Characteristics of Worn Surface

A high-carbon, high-silicon steel (1.21 wt% C, 2.56 wt% Mn, 1.59 wt% Si) was subjected to quenching from 900 and 1000 °C, resulting in microstructures containing 60 and 94% of retained austenite, respectively. Subsequent abrasive wear tests of quenched samples were performed using two-body abrasion...