Cargando…

Statistically Optimum HKUST-1 Synthesized by Room Temperature Coordination Modulation Method for the Adsorption of Crystal Violet Dye

Due to its excellency and versatility, many synthesis methods and conditions were developed to produce HKUST-1 ([Cu(3)(BTC)(2)(H(2)O)(3)](n)). However, the diversity of HKUST-1 was actually generated both in terms of characteristics and morphologies. Hence, the consistency of HKUST-1 characteristics...

Descripción completa

Detalles Bibliográficos
Autores principales: Wijaya, Christian J., Ismadji, Suryadi, Aparamarta, Hakun W., Gunawan, Setiyo
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8588197/
https://www.ncbi.nlm.nih.gov/pubmed/34770838
http://dx.doi.org/10.3390/molecules26216430
Descripción
Sumario:Due to its excellency and versatility, many synthesis methods and conditions were developed to produce HKUST-1 ([Cu(3)(BTC)(2)(H(2)O)(3)](n)). However, the diversity of HKUST-1 was actually generated both in terms of characteristics and morphologies. Hence, the consistency of HKUST-1 characteristics and morphologies needs to be maintained. The statistical analysis and optimization provide features to determine the best synthesis condition. Here, a room-temperature coordination modulation method was proposed to maintain the morphology of HKUST-1 while reducing energy consumption. In addition, response surface methodology (RSM) was used to demonstrate the statistical analysis and optimization of the synthesis of HKUST-1. The molar ratio of ligand to metal, reaction time, and acetic acid concentration were studied to determine their effects on HKUST-1. The optimum HKUST-1 was obtained by the synthesis with a molar ratio of ligand to metal of 0.4703 for 27.2 h using 5% v/v acetic acid concentration. The statistical analysis performed a good agreement with the experimental data and showed the significance of three desired parameters on HKUST-1. The optimum HKUST-1 had the adsorption capacity of 1005.22 mg/g with a removal efficiency of 92.31% towards CV dye. It could be reused up to 5 cycles with insignificant decrease in performance.