Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials
Silicon (Si) containing materials cannot be used in commercial lithium ion batteries due to the mechanical stress problem triggered by volume expansion during cycling. The high-volume change causes mechanical instability of Si anode materials during charging/discharging, resulting fast capacity fadi...
Autores principales: | , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Scientific and Technological Research Council of Turkey
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8596531/ https://www.ncbi.nlm.nih.gov/pubmed/34849065 http://dx.doi.org/10.3906/kim-2102-62 |
_version_ | 1784600399010856960 |
---|---|
author | DOĞRUSÖZ, Mehbare DEMİRKAN, M. Taha DEMİR-ÇAKAN, Rezan |
author_facet | DOĞRUSÖZ, Mehbare DEMİRKAN, M. Taha DEMİR-ÇAKAN, Rezan |
author_sort | DOĞRUSÖZ, Mehbare |
collection | PubMed |
description | Silicon (Si) containing materials cannot be used in commercial lithium ion batteries due to the mechanical stress problem triggered by volume expansion during cycling. The high-volume change causes mechanical instability of Si anode materials during charging/discharging, resulting fast capacity fading. It is thought that piezoelectric materials can be a solution for the volume expansion problem because of their ability to generate electric field when pressure is applied on them. For this purpose, PZT-8 and PZT-5H type piezoelectric materials were mixed with silicon and multiwalled carbon nanotube (MWCNT) to obtain anode composites and tested electrochemically versus lithium metal. The piezoelectiric effect on the electrochemical activity of these anodes is investigated by preparing the anode composite without any piezoelectric material additive (Sample #3). At the end of the 50 charge/discharge cycles, the capacities reached 420 mAh/g, 300 mAh/g and 100 mAh/g for PZT-8-added, PZT-5H-added and no-PZT samples, respectively. These results showed that PZT addition improves capacity performance of Si-MWCNT anodes. Additionally, the obtained anode composites were characterized with X-ray diffraction and scanning electron microscopy. |
format | Online Article Text |
id | pubmed-8596531 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2021 |
publisher | The Scientific and Technological Research Council of Turkey |
record_format | MEDLINE/PubMed |
spelling | pubmed-85965312021-11-29 Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials DOĞRUSÖZ, Mehbare DEMİRKAN, M. Taha DEMİR-ÇAKAN, Rezan Turk J Chem Article Silicon (Si) containing materials cannot be used in commercial lithium ion batteries due to the mechanical stress problem triggered by volume expansion during cycling. The high-volume change causes mechanical instability of Si anode materials during charging/discharging, resulting fast capacity fading. It is thought that piezoelectric materials can be a solution for the volume expansion problem because of their ability to generate electric field when pressure is applied on them. For this purpose, PZT-8 and PZT-5H type piezoelectric materials were mixed with silicon and multiwalled carbon nanotube (MWCNT) to obtain anode composites and tested electrochemically versus lithium metal. The piezoelectiric effect on the electrochemical activity of these anodes is investigated by preparing the anode composite without any piezoelectric material additive (Sample #3). At the end of the 50 charge/discharge cycles, the capacities reached 420 mAh/g, 300 mAh/g and 100 mAh/g for PZT-8-added, PZT-5H-added and no-PZT samples, respectively. These results showed that PZT addition improves capacity performance of Si-MWCNT anodes. Additionally, the obtained anode composites were characterized with X-ray diffraction and scanning electron microscopy. The Scientific and Technological Research Council of Turkey 2021-10-19 /pmc/articles/PMC8596531/ /pubmed/34849065 http://dx.doi.org/10.3906/kim-2102-62 Text en Copyright © 2021 The Author(s) https://creativecommons.org/licenses/by/4.0/This article is distributed under the terms of the Creative Commons Attribution License (http://creativecommons.org/licenses/by/4.0/ (https://creativecommons.org/licenses/by/4.0/) ), which permits unrestricted use and redistribution provided that the original author and source are credited. |
spellingShingle | Article DOĞRUSÖZ, Mehbare DEMİRKAN, M. Taha DEMİR-ÇAKAN, Rezan Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials |
title | Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials |
title_full | Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials |
title_fullStr | Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials |
title_full_unstemmed | Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials |
title_short | Investigation of PZT-5H and PZT-8 type piezoelectric effect on cycling stability on Si-MWCNT containing anode materials |
title_sort | investigation of pzt-5h and pzt-8 type piezoelectric effect on cycling stability on si-mwcnt containing anode materials |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8596531/ https://www.ncbi.nlm.nih.gov/pubmed/34849065 http://dx.doi.org/10.3906/kim-2102-62 |
work_keys_str_mv | AT dogrusozmehbare investigationofpzt5handpzt8typepiezoelectriceffectoncyclingstabilityonsimwcntcontaininganodematerials AT demirkanmtaha investigationofpzt5handpzt8typepiezoelectriceffectoncyclingstabilityonsimwcntcontaininganodematerials AT demircakanrezan investigationofpzt5handpzt8typepiezoelectriceffectoncyclingstabilityonsimwcntcontaininganodematerials |