Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting

In this study, the wear behavior of a heat-treatable Al-7Si-0.5Mg-0.5Cu alloy fabricated by selective laser melting was investigated systematically. Compared with the commercial homogenized AA2024 alloy, the fine secondary phase of the SLM Al-Cu-Mg-Si alloy leads to a low specific wear rate (1.8 ± 0...

Descripción completa

Detalles Bibliográficos
Autores principales: Wang, Pei, Lei, Yang, Qi, Jun-Fang, Yu, Si-Jie, Setchi, Rossitza, Wu, Ming-Wei, Eckert, Jürgen, Li, Hai-Chao, Scudino, Sergio
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8620008/
https://www.ncbi.nlm.nih.gov/pubmed/34832447
http://dx.doi.org/10.3390/ma14227048
_version_ 1784605121514045440
author Wang, Pei
Lei, Yang
Qi, Jun-Fang
Yu, Si-Jie
Setchi, Rossitza
Wu, Ming-Wei
Eckert, Jürgen
Li, Hai-Chao
Scudino, Sergio
author_facet Wang, Pei
Lei, Yang
Qi, Jun-Fang
Yu, Si-Jie
Setchi, Rossitza
Wu, Ming-Wei
Eckert, Jürgen
Li, Hai-Chao
Scudino, Sergio
author_sort Wang, Pei
collection PubMed
description In this study, the wear behavior of a heat-treatable Al-7Si-0.5Mg-0.5Cu alloy fabricated by selective laser melting was investigated systematically. Compared with the commercial homogenized AA2024 alloy, the fine secondary phase of the SLM Al-Cu-Mg-Si alloy leads to a low specific wear rate (1.8 ± 0.11 × 10(−4) mm(3)(Nm)(−1)) and a low average coefficient of friction (0.40 ± 0.01). After the T6 heat treatment, the SLM Al-Cu-Mg-Si alloy exhibits a lower specific wear rate (1.48 ± 0.02 × 10(−4) mm(3)(Nm)(−1)), but a similar average coefficient of friction (0.34 ± 0.01) as the heat-treated AA2024 alloy. Altogether, the SLM Al-3.5Cu-1.5Mg-1Si alloy is suitable for the achievement of not only superior mechanical performance, but also improved tribological properties.
format Online
Article
Text
id pubmed-8620008
institution National Center for Biotechnology Information
language English
publishDate 2021
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-86200082021-11-27 Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting Wang, Pei Lei, Yang Qi, Jun-Fang Yu, Si-Jie Setchi, Rossitza Wu, Ming-Wei Eckert, Jürgen Li, Hai-Chao Scudino, Sergio Materials (Basel) Article In this study, the wear behavior of a heat-treatable Al-7Si-0.5Mg-0.5Cu alloy fabricated by selective laser melting was investigated systematically. Compared with the commercial homogenized AA2024 alloy, the fine secondary phase of the SLM Al-Cu-Mg-Si alloy leads to a low specific wear rate (1.8 ± 0.11 × 10(−4) mm(3)(Nm)(−1)) and a low average coefficient of friction (0.40 ± 0.01). After the T6 heat treatment, the SLM Al-Cu-Mg-Si alloy exhibits a lower specific wear rate (1.48 ± 0.02 × 10(−4) mm(3)(Nm)(−1)), but a similar average coefficient of friction (0.34 ± 0.01) as the heat-treated AA2024 alloy. Altogether, the SLM Al-3.5Cu-1.5Mg-1Si alloy is suitable for the achievement of not only superior mechanical performance, but also improved tribological properties. MDPI 2021-11-20 /pmc/articles/PMC8620008/ /pubmed/34832447 http://dx.doi.org/10.3390/ma14227048 Text en © 2021 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Wang, Pei
Lei, Yang
Qi, Jun-Fang
Yu, Si-Jie
Setchi, Rossitza
Wu, Ming-Wei
Eckert, Jürgen
Li, Hai-Chao
Scudino, Sergio
Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting
title Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting
title_full Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting
title_fullStr Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting
title_full_unstemmed Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting
title_short Wear Behavior of a Heat-Treatable Al-3.5Cu-1.5Mg-1Si Alloy Manufactured by Selective Laser Melting
title_sort wear behavior of a heat-treatable al-3.5cu-1.5mg-1si alloy manufactured by selective laser melting
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8620008/
https://www.ncbi.nlm.nih.gov/pubmed/34832447
http://dx.doi.org/10.3390/ma14227048
work_keys_str_mv AT wangpei wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT leiyang wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT qijunfang wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT yusijie wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT setchirossitza wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT wumingwei wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT eckertjurgen wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT lihaichao wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting
AT scudinosergio wearbehaviorofaheattreatableal35cu15mg1sialloymanufacturedbyselectivelasermelting