Cargando…
The Effect of Deposited Dust on SCC and Crevice Corrosion of AISI 304L Stainless Steel in Saline Environment
Crevice corrosion has become an important issue of the safety of AISI 304L austenitic stainless steel canister when exposed to the chloride environments located in coastal areas. Moreover, dust deposited on the canister surface may enhance the corrosion effect of 304L stainless steel. In this work,...
Autores principales: | Yeh, Chun-Ping, Tsai, Kun-Chao, Huang, Jiunn-Yuan |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8622586/ https://www.ncbi.nlm.nih.gov/pubmed/34832235 http://dx.doi.org/10.3390/ma14226834 |
Ejemplares similares
-
The Corrosion Susceptibility of 304L Stainless Steel Exposed to Crevice Environments
por: Tsai, Kun-Chao, et al.
Publicado: (2022) -
Influence of Chloride Concentration on Stress Corrosion Cracking and Crevice Corrosion of Austenitic Stainless Steel in Saline Environments
por: Yeh, Chun-Ping, et al.
Publicado: (2020) -
Effect of Cathodic Polarisation Switch-Off on the Passivity and Stability to Crevice Corrosion of AISI 304L Stainless Steel
por: Shubina Helbert, Varvara, et al.
Publicado: (2021) -
Effect of Heat Treatment on Crevice Corrosion Behavior of 304 Stainless Steel Clad Plate in Seawater Environment
por: Hang, Pengwei, et al.
Publicado: (2023) -
Corrosion Behavior of Sensitized AISI 304 Stainless Steel in Acid Chloride Solution
por: Zatkalíková, Viera, et al.
Publicado: (2022)