Evaluation of the Performance and Ductility Index of Concrete Structures Using Advanced Composite Material Strengthening Methods

The performance of concrete structures deteriorates over time. Thus, improving their performance using fiber-reinforced polymers (FRPs), PS strands, and various strengthening methods is important. Reinforced concrete (RC) and prestressed concrete (PSC) structures develop initial cracks in concrete d...

Descripción completa

Detalles Bibliográficos
Autores principales: Kim, Tae-Kyun, Park, Jong-Sup
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8659728/
https://www.ncbi.nlm.nih.gov/pubmed/34883742
http://dx.doi.org/10.3390/polym13234239
Descripción
Sumario:The performance of concrete structures deteriorates over time. Thus, improving their performance using fiber-reinforced polymers (FRPs), PS strands, and various strengthening methods is important. Reinforced concrete (RC) and prestressed concrete (PSC) structures develop initial cracks in concrete during bending tests, and destruction occurs over a certain period of time after a certain load is generated, and then after the reinforcements and strands yield. However, in the case of FRP structures, after an initial concrete crack occurs, FRPs exhibit a rapid shape deformation of the structure after yielding. Thus, in this study we used FRP and PS strand materials and evaluated the ductility index using the load-displacement results obtained from structural tests conducted using various strengthening methods. The ductility index evaluation method compares and analyzes the change rates in the ductility index of PSC and RC structures based on a method that uses structural deflection and the derivation of the energy area ratio. The ductility evaluation results based on the energy area ratio at the crack, yield, and ultimate points showed that all the RC structures, except for the specimens strengthened with reinforcing materials from company H, were in the ductility and semi-ductility sections. Thus, all the PSC structures, except for the control specimens and PH4NP, were found to be brittle.