About the transformation of low T(m) into high T(m) poly(l-lactide)s by annealing under the influence of transesterification catalysts

Cyclic polylactides were prepared in bulk at 170 °C, crystallized at 120 °C and then annealed at temperatures between 130 and 170 °C with variation of catalyst, catalyst concentration and annealing time. The transformation of the initially formed low melting (LT(m)) crystallites, having melting temp...