Atomic layer deposition of superparamagnetic ruthenium-doped iron oxide thin film

Due to the several applications of biosensors, such as magnetic hyperthermia and magnetic resonance imaging, the use of superparamagnetic nanoparticles or thin films for preparing biosensors has increased greatly. We report herein on a strategy to fabricate a nanostructure composed of superparamagne...

Descripción completa

Detalles Bibliográficos
Autores principales: Tamm, Aile, Tarre, Aivar, Kozlova, Jekaterina, Rähn, Mihkel, Jõgiaas, Taivo, Kahro, Tauno, Link, Joosep, Stern, Raivo
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Royal Society of Chemistry 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8694953/
https://www.ncbi.nlm.nih.gov/pubmed/35423279
http://dx.doi.org/10.1039/d1ra00507c
Descripción
Sumario:Due to the several applications of biosensors, such as magnetic hyperthermia and magnetic resonance imaging, the use of superparamagnetic nanoparticles or thin films for preparing biosensors has increased greatly. We report herein on a strategy to fabricate a nanostructure composed of superparamagnetic thin films. Ruthenium-doped iron oxide thin films were deposited by using atomic layer deposition at 270 and 360 °C. FeCl(3) and Ru(EtCp)(2) were used as metal precursors and H(2)O/O(2) as the oxygen precursor. Doping with ruthenium helps to lower the formation temperature of hematite (α-Fe(2)O(3)). Ruthenium content was changed from 0.42 at% up to 29.7 at%. Ru-doped films had a nano-crystallized structure of hematite with nanocrystal sizes from 4.4 up to 7.8 nm. Magnetization at room temperature was studied in iron oxide and Ru-doped iron oxide films. A new finding is a demonstration that in a Ru-doped iron oxide thin film superparamagnetic behavior of nanocrystalline materials (α-Fe(2)O(3)) is observed with the maximum magnetic coercive force H(c) of 3 kOe. Increasing Ru content increased crystallite size of hematite and resulted in a lower blocking temperature.