Preparation and anti-coking application of sol–gel SiO(2) coating in a delayed coking furnace
To isolate iron sulphide and reduce coke adhesion reactions that occur on the surface of a delayed coking furnace, a SiO(2) coating was developed on Cr9Mo alloy by employing the sol–gel method. The coating was characterised through Fourier transformation infrared spectroscopy, X-ray diffraction, sca...
Autores principales: | Liu, Jinglei, Wang, Xiangxiang, Wang, Hao, Xu, Hong, Yang, Jiangfeng |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Royal Society of Chemistry
2021
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8695414/ https://www.ncbi.nlm.nih.gov/pubmed/35423529 http://dx.doi.org/10.1039/d1ra00237f |
Ejemplares similares
-
Gas Furnaces vs. Coal or Coke
por: Land, H. C.
Publicado: (1886) -
Gas Furnaces vs. Coal or Coke
por: Land, H. C.
Publicado: (1886) -
Experimental research on semi-coke for blast furnace injection
por: Huang, Chun-chao, et al.
Publicado: (2020) -
Calculation of Coke Layers Situation in the Cohesive Zone of Blast Furnace
por: Bernasowski, Mikolaj, et al.
Publicado: (2021) -
Influence of Zinc on Nonisothermal Gasification Kinetics
of Coke in a Blast Furnace
por: Wang, Jie, et al.
Publicado: (2021)