Cargando…

Low-Carbon and Fundamental Properties of Eco-Efficient Mortar with Recycled Powders

Using recycled powders from solid waste is accepted as an effective strategy to realize the sustainable development of the construction industry. In our study, the cement was substituted by two kinds of recycled powders, i.e., spontaneous combustion gangue powder (SCGP) and recycled concrete powder...

Descripción completa

Detalles Bibliográficos
Autores principales: Sun, Chang, Chen, Lulu, Xiao, Jianzhuang, Liu, Qiong, Zuo, Junqing
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2021
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8704208/
https://www.ncbi.nlm.nih.gov/pubmed/34947099
http://dx.doi.org/10.3390/ma14247503
Descripción
Sumario:Using recycled powders from solid waste is accepted as an effective strategy to realize the sustainable development of the construction industry. In our study, the cement was substituted by two kinds of recycled powders, i.e., spontaneous combustion gangue powder (SCGP) and recycled concrete powder (RCP), with a certain replacement ratio of 30%. The experimental variables were mainly the type of replacement powder (e.g., SCGP, RCP, and SCGP + RCP) and the grinding time of RCP (e.g., 25 min, 50 min, and 75 min). The fundamental properties, including mechanical properties, long-term properties, and carbon emission, were analyzed for all the mortar mixtures. Experimental results indicate that incorporation of RCP contributes to enhancing the toughness and dry shrinkage resistance of eco-efficient mortar, while SCGP positively affects the compressive strength and chloride resistance. The grinding process improves the activity of RCP to a certain extent, while a long grinding time leads to fusion and aggregation between powders. Investigation on CO(2) emission demonstrates that carbon emission from cement production accounts for the largest proportion, 80~95%, in the total emission from mortar production. Combined with the AHP model, eco-efficient mortar containing 15% RCP ground for 50 min and 15% SCGP displays optimal fundamental properties.