Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc
This paper presents studies on the processing of enrichment tailings as a component of a raw mixture in order to obtain cement clinker, with simultaneous distillation of zinc. Thermodynamic studies were carried out in the temperature range of 600–1600 °C using the software application “HSC Chemistry...
Autores principales: | , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8746131/ https://www.ncbi.nlm.nih.gov/pubmed/35009470 http://dx.doi.org/10.3390/ma15010324 |
_version_ | 1784630511148204032 |
---|---|
author | Kolesnikov, Alexandr Fediuk, Roman Kolesnikova, Olga Zhanikulov, Nurgali Zhakipbayev, Bibol Kuraev, Rasim Akhmetova, Elmira Shal, Aizhan |
author_facet | Kolesnikov, Alexandr Fediuk, Roman Kolesnikova, Olga Zhanikulov, Nurgali Zhakipbayev, Bibol Kuraev, Rasim Akhmetova, Elmira Shal, Aizhan |
author_sort | Kolesnikov, Alexandr |
collection | PubMed |
description | This paper presents studies on the processing of enrichment tailings as a component of a raw mixture in order to obtain cement clinker, with simultaneous distillation of zinc. Thermodynamic studies were carried out in the temperature range of 600–1600 °C using the software application “HSC Chemistry 6” developed by the metallurgical company Outokumpu (Finland). As a result of the conducted studies, we found that zinc contributes to the intensification of mineral formation of cement clinker. In particular, it was found that the formation of belite is possible in the temperature range from 990.7 to 1500 °C with Gibbs energy values of −0.01 and −323.8 kJ (which is better than the standard process by −11.4 kJ), respectively; the formation of alite is possible in the temperature range from 982.9 to 1500 °C with Gibbs energy values of −0.05 and −402.1 kJ (better than the standard process by −11.4 kJ), respectively; the formation of tricalcium aluminate is thermodynamically possible in the temperature range from 600 °C at ΔG(T)(o) = −893.8 kJ to 1500 °C at ΔG(T)(o) = −1899.3 kJ (better than the standard process by −1570.1 kJ), respectively; and the formation of four calcium aluminoferrite is possible in the temperature range from 600 °C at ΔG(T)(o) = −898.9 kJ to 1500 °C at ΔG(T)(o) = −1959.3 kJ (better than the standard process by −1570.2 kJ), respectively, with simultaneous distillation of zinc into a gaseous state for its further capture. |
format | Online Article Text |
id | pubmed-8746131 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2022 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-87461312022-01-11 Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc Kolesnikov, Alexandr Fediuk, Roman Kolesnikova, Olga Zhanikulov, Nurgali Zhakipbayev, Bibol Kuraev, Rasim Akhmetova, Elmira Shal, Aizhan Materials (Basel) Article This paper presents studies on the processing of enrichment tailings as a component of a raw mixture in order to obtain cement clinker, with simultaneous distillation of zinc. Thermodynamic studies were carried out in the temperature range of 600–1600 °C using the software application “HSC Chemistry 6” developed by the metallurgical company Outokumpu (Finland). As a result of the conducted studies, we found that zinc contributes to the intensification of mineral formation of cement clinker. In particular, it was found that the formation of belite is possible in the temperature range from 990.7 to 1500 °C with Gibbs energy values of −0.01 and −323.8 kJ (which is better than the standard process by −11.4 kJ), respectively; the formation of alite is possible in the temperature range from 982.9 to 1500 °C with Gibbs energy values of −0.05 and −402.1 kJ (better than the standard process by −11.4 kJ), respectively; the formation of tricalcium aluminate is thermodynamically possible in the temperature range from 600 °C at ΔG(T)(o) = −893.8 kJ to 1500 °C at ΔG(T)(o) = −1899.3 kJ (better than the standard process by −1570.1 kJ), respectively; and the formation of four calcium aluminoferrite is possible in the temperature range from 600 °C at ΔG(T)(o) = −898.9 kJ to 1500 °C at ΔG(T)(o) = −1959.3 kJ (better than the standard process by −1570.2 kJ), respectively, with simultaneous distillation of zinc into a gaseous state for its further capture. MDPI 2022-01-03 /pmc/articles/PMC8746131/ /pubmed/35009470 http://dx.doi.org/10.3390/ma15010324 Text en © 2022 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Kolesnikov, Alexandr Fediuk, Roman Kolesnikova, Olga Zhanikulov, Nurgali Zhakipbayev, Bibol Kuraev, Rasim Akhmetova, Elmira Shal, Aizhan Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc |
title | Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc |
title_full | Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc |
title_fullStr | Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc |
title_full_unstemmed | Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc |
title_short | Processing of Waste from Enrichment with the Production of Cement Clinker and the Extraction of Zinc |
title_sort | processing of waste from enrichment with the production of cement clinker and the extraction of zinc |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8746131/ https://www.ncbi.nlm.nih.gov/pubmed/35009470 http://dx.doi.org/10.3390/ma15010324 |
work_keys_str_mv | AT kolesnikovalexandr processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc AT fediukroman processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc AT kolesnikovaolga processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc AT zhanikulovnurgali processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc AT zhakipbayevbibol processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc AT kuraevrasim processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc AT akhmetovaelmira processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc AT shalaizhan processingofwastefromenrichmentwiththeproductionofcementclinkerandtheextractionofzinc |