[Image: see text] X-ray scintillation detectors based on metal halide perovskites have shown excellent light yield, but they mostly target applications with spatial resolution at the tens of micrometers level. Here, we use a one-step solution method to grow arrays of 15-μm-long single-crystalline Cs...

Descripción completa

Detalles Bibliográficos
Autores principales: Zhang, Zhaojun, Dierks, Hanna, Lamers, Nils, Sun, Chen, Nováková, Klára, Hetherington, Crispin, Scheblykin, Ivan G., Wallentin, Jesper
Formato: Online Artículo Texto
Lenguaje:English
Publicado: American Chemical Society 2021
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8805114/
https://www.ncbi.nlm.nih.gov/pubmed/35128340
http://dx.doi.org/10.1021/acsanm.1c03575
Descripción
Sumario:[Image: see text] X-ray scintillation detectors based on metal halide perovskites have shown excellent light yield, but they mostly target applications with spatial resolution at the tens of micrometers level. Here, we use a one-step solution method to grow arrays of 15-μm-long single-crystalline CsPbBr(3) nanowires (NWs) in an AAO (anodized aluminum oxide) membrane template, with nanowire diameters ranging from 30 to 360 nm. The CsPbBr(3) nanowires in AAO (CsPbBr(3) NW/AAO) show increasing X-ray scintillation efficiency with decreasing nanowire diameter, with a maximum photon yield of ∼5 300 ph/MeV at 30 nm diameter. The CsPbBr(3) NW/AAO composites also display high radiation resistance, with a scintillation-intensity decrease of only ∼20–30% after 24 h of X-ray exposure (integrated dose 162 Gy(air)) and almost no change after ambient storage for 2 months. X-ray images can distinguish line pairs with a spacing of 2 μm for all nanowire diameters, while slanted edge measurements show a spatial resolution of ∼160 lp/mm at modulation transfer function (MTF) = 0.1. The combination of high spatial resolution, radiation stability, and easy fabrication makes these CsPbBr(3) NW/AAO scintillators a promising candidate for high-resolution X-ray imaging applications.