Effect of the Flame Retardants and Glass Fiber on the Polyamide 66/Polyphenylene Oxide Composites
In this work, polyamide 66/polyphenylene oxide (PA66/PPO) composites, including the flame retardants 98 wt% aluminum diethylphosphinate + 2 wt% polydimethylsiloxane (P@Si), Al(OH)(3)-coated red phosphorus (RP*), and glass fiber (GF), were systematically studied, respectively. The limiting oxygen ind...
Autores principales: | , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2022
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC8837021/ https://www.ncbi.nlm.nih.gov/pubmed/35160757 http://dx.doi.org/10.3390/ma15030813 |
Sumario: | In this work, polyamide 66/polyphenylene oxide (PA66/PPO) composites, including the flame retardants 98 wt% aluminum diethylphosphinate + 2 wt% polydimethylsiloxane (P@Si), Al(OH)(3)-coated red phosphorus (RP*), and glass fiber (GF), were systematically studied, respectively. The limiting oxygen index (LOI), UL-94 vertical burning level, and thermal and mechanical properties of the PA66/PPO composites were characterized. The results showed that the P@Si and RP flame retardants both improved the LOI value and UL-94 vertical burning level of the PA66/PPO composites, and PA66/PPO composites passed to the UL-94 V-0 level when the contents of P@Si and RP* flame retardants were 16 wt% and 8 wt%. On the other hand, the mechanical properties of the PA66/PPO composites were reduced from a ductile to a brittle fracture mode. The addition of GF effectively made up for these defects and improved the mechanical properties of the PA66/PPO composites containing the P@Si and RP*, but it did not change the fracture mode. P@Si and RP* flame retardants improved the thermal decomposition of PA66/PPO/GF composites and reduced the maximum mass loss rates, showing that the PA66/PPO/GF composites containing the P@Si and RP* flame retardants could be used in higher-temperature fields. |
---|